US 9,922,808 B2#31771243 Most CitedActiveUnited States (USPTO)Utility

Multi-block sputtering target and associated methods and articles

3Forward Citations (#31771243 Global)
0.4/yrCitation Velocity (#21440132 Global)
1.14Citation PageRank (#34995190 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A sputtering target that includes at least two consolidated blocks, each block including an alloy including molybdenum in an amount greater than about 30 percent by weight and at least one additional alloying ingredient; and a joint between the at least two consolidated blocks, the joint being free of any microstructure due to an added bonding agent (e.g., powder, foil or otherwise), and being essentially free of any visible joint line the target that is greater than about 200 μm width (e.g., less than about 50 μm width). A process for making the target includes hot isostatically pressing, below a temperature of 1080° C., consolidated perform blocks that may be surface prepared (e.g., roughened to a predetermined roughness value) prior to pressing.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A sputtering target, comprising: a) at least two consolidated blocks, each block including an alloy including molybdenum in an amount greater than about 30 percent by weight and at least one additional alloying element; and b) a joint between the at least two consolidated blocks, which joins the blocks together to define a target body, the joint being free of any microstructure due to an added bonding agent, and being essentially free of any joint line of greater than about 300 μm width, wherein the sputtering target at the joint exhibits a transverse rupture strength per ASTM B528-10, of at l

  2. Claim 2Depends on #1

    The sputtering target of claim 1 , wherein the consolidated joint is essentially free of any joint line greater than 200 μm width and provides a structure that has a transverse rupture strength per ASTM B528-10, of at le

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,714,702 AMethod for diffusion bonding refractory metals and alloys197335
US 4,208,257 AMethod of forming an interconnection198029
US 4,647,426 AProduction of billet and extruded products from particulate materials198727
US 4,747,907 AMetal etching process with etch rate enhancement198857
EP 0,285,130 A1Sputtering target—18
US 4,820,393 ATitanium nitride sputter targets198952
US 4,938,798 ASputtering target and process for preparing the same199054
EP 0,590,904 A1Diffusion-bonded sputtering target assembly and method of manufacturing the same—57
JP H06177085 AFormation of wiring—12
JP H06264233 ASputtering target for producing tft—15
US 5,397,050 AMethod of bonding tungsten titanium sputter targets to titanium plates and target assemblies produced thereby199590
US 5,429,877 AInternally reinforced hollow titanium alloy components199582
US 5,435,965 ASputtering target and method for manufacturing same199596
US 5,733,427 ASputtering target and method of manufacturing the same199824
US 5,857,611 ASputter target/backing plate assembly and method of making same199931
JP H1174218 ASemiconductor device and its manufacture—15
EP 0,902,102 A1Ta sputtering targets, method of manufacturing the same, and assemblies—63
US 5,895,663 APseudoephedrine hydrochloride extended-release tablets199944
US 5,896,553 ASingle phase tungsten-titanium sputter targets and method of producing same199928
JP H11246967 ATarget for irmn series alloy film formation, its production and antiferromagnetic film using it—10
US 5,963,778 AMethod for producing near net shape planar sputtering targets and an intermediate therefor199941
US 6,010,583 AMethod of making unreacted metal/aluminum sputter target200040
US 6,042,777 AManufacturing of high density intermetallic sputter targets200045
US 6,071,389 ADiffusion bonded sputter target assembly and method of making2000149
JP 2000239838 ASputtering target assembled body subjected to solid phase diffusion joining and its production—30
US 6,159,625 ATarget of intermetallic compound with B2-ordered lattice structure, production method thereof and magnetic recording medium having B2-structured underlayer200056
US 6,165,413 AMethod of making high density sputtering targets200041

Non-Patent Literature (5)

  • Chinese Office Action dated Jan. 22, 2010 (in Chinese).
  • Chinese Office Action dated Jan. 22, 2010 tranlated by Chinese Agent, Shanghai Patent & Trademark Law Office, LLC on Feb. 25, 2010.
  • Contribute to the Development of Light Metal through Encouragement and Promotion of Reseach Study Education, Published in Surface and Coating Technology, vol. 169-170, pp. 151-154, (month unavailable) 2003, H. Habazaki et al., “Formation of Barrier-type Amorphous Anodic Films on Ti—Mo Alloys,” pp. 1
  • Copending U.S. Appl. No. 12/090,919, filed Jul. 11, 2008, entitled, “Methods of Making Molybdenum”, Applicant Gaydos, et al. (Publication: US2008/0314737 A1 on Dec. 25, 2008).
  • Copending U.S. Appl. No. 12/917,668, filed Nov. 2, 2010, entitled, “Methods of Making Molybdenum”, Applicant Gaydos, et al. (Publication: US2011/0097236 on Apr. 28, 2011).