Removal of ferric iron as hematite at atmospheric pressure
Abstract
A process for the removal of ferric iron as hematite from a nickel solution containing ferric and ferrous ions including the steps of: raising the temperature of the nickel solution to between 90° C. and the boiling point of the solution at atmospheric pressure; raising the pH of the nickel solution to be between 2 and 3; and adding a hematite seed to facilitate hematite precipitation, wherein ferric ions are precipitated as hematite in a predominantly crystalline form.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for the removal of ferric iron as hematite from a nickel solution containing ferric and ferrous ions including the sequential steps of: (i) raising the temperature of the nickel solution to between about 90° C. and the boiling point of the nickel solution at atmospheric pressure; (ii) adjusting the pH of the nickel solution to be between about 2 and about 3; and (iii) adding a hematite seed to precipitate ferric ions as hematite in a predominantly crystalline form and to form a solution substantially free of ferric ions; (iv) recovering nickel from the solution substantially free of
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (5)
Non-Patent Literature (1)
- PCT/AU2013/000666 International Search Report dated Oct. 1, 2013 (3 pages).