Large area format sapphire windows via transient liquid phase bonding
Abstract
A method for forming an optical window. In one example, the method includes depositing a layer of eutectic bonding material onto a first surface of a first section of window material, positioning a second surface of a second section of window material onto the layer of eutectic bonding material such that the first surface is disposed opposite the second surface, and heating the eutectic bonding material to a temperature above a eutectic temperature of the eutectic bonding material and below a melting temperature of the window material for a predetermined length of time to form an optical window. The window material of the first section and the second section may be transparent to infrared radiation and comprise aluminum.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of forming an optical window comprising: depositing a layer of eutectic bonding material onto a first surface of a first section of a window material, wherein the eutectic bonding material is an aluminosilicate; positioning a second surface of a second section of the window material onto the layer of eutectic bonding material such that the first surface is disposed opposite the second surface, the window material being transparent to infrared radiation and including aluminum; and heating the eutectic bonding material to a temperature above a eutectic temperature of the eutectic bondin
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 10,793,970 B2 | Method of fabricating a turbine engine part | 2020 | 0 |