Fusion formable glass-based articles including a metal oxide concentration gradient
Abstract
A glass-based article including a first surface and a second surface opposing the first surface defining a thickness (t) of about 3 millimeters or less (e.g., about 1 millimeter or less), and a stress profile, wherein all points of the stress profile between a thickness range from about 0·t up to 0.3·t and from greater than about 0.7·t to t, comprise a tangent with a slope having an absolute value greater than about 0.1 MPa/micrometer. In some embodiments, the glass-based article includes a non-zero metal oxide concentration that varies along at least a portion of the thickness (e.g., 0·t to about 0.3·t) and a maximum central tension of less than about 71.5/√(t) (MPa). In some embodiments, the concentration of metal oxide or alkali metal oxide decreases from the first surface to a point between the first surface and the second surface and increases from the point to the second surface. The concentration of the metal oxide may be about 0.05 mol % or greater or about 0.5 mol % or greater throughout the thickness. Methods for forming such glass-based articles are also disclosed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 11.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A glass-based article comprising: a first surface and a second surface opposing the first surface defining a thickness (t) (mm); a concentration of a metal oxide that is both non-zero and varies along a thickness range from about 0•t to about 0.3•t; a surface compressive stress of about 200 MPa or greater; and a central tension (CT) region comprising a maximum CT (MPa) of less than about 71.5/√(t).
- Claim 2Depends on #1
The glass-based article of claim 1 , wherein the concentration of the metal oxide is non-zero and varies along the entire thickness.
- Claim 3Depends on #1
The glass-based article of claim 1 , comprising: a first metal oxide concentration and a second metal oxide concentration, wherein the first metal oxide concentration varies in a range from about 15 mol % to about 0 mol % as thickness varies over a first range from ab
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗