Abstract
A method is provided for forming an ultra-shallow boron doping region in a semiconductor device. The method includes depositing a diffusion filter layer on a substrate, the diffusion filter containing a boron nitride layer, a boron oxynitride layer, a silicon nitride layer, or a silicon oxynitride layer, and depositing a boron dopant layer on the diffusion filter layer, the boron dopant layer containing boron oxide, boron oxynitride, or a combination thereof, with the proviso that the diffusion filter layer and the boron dopant layer do not contain the same material. The method further includes heat-treating the substrate to form the ultra-shallow boron dopant region in the substrate by controlled diffusion of boron from the boron dopant layer through the diffusion filter layer and into the substrate.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 46 · Forward citations: 3.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of forming an ultra-shallow boron doping region in a semiconductor device, the method comprising: depositing a diffusion filter layer on a substrate, the diffusion filter layer containing a boron nitride layer, a boron oxynitride layer, a silicon nitride layer, or a silicon oxynitride layer; depositing a boron dopant layer on the diffusion filter layer, the boron dopant layer containing boron oxide, boron oxynitride, or a combination thereof, with the proviso that the diffusion filter layer and the boron dopant layer do not contain the same material; and heat-treating the substrate to
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 11,443,948 B2 | Doping techniques | 2022 | 0 |
| US 12,421,604 B2 | Ultra-shallow dopant and ohmic contact regions by solid state diffusion | 2025 | 0 |
| US 12,261,047 B2 | Doping techniques | 2025 | 0 |
References Cited — Backward Prior Art (46)
Non-Patent Literature (5)
- Ho et al. “Wafer-Scale, Sub-5 nm Junction Formation by Monolayer Doping and Conventional Spike Annealing,” Nano Letter, 95 (2) (2009) 725-730.
- Kalkofen et al. “Atomic layer deposition of boron oxide as dopant source for shallow doping of silicon”, 217th Electrochemical Society Meeting Abstract #943, Vancouver, Canada, Apr. 25-30, 2010, 1 page.
- Kalkofen et al. “P-type Doping of Silicon Suitable for Structures with High Aspect Ratios by Using a Dopant Source of Boron Oxide Grown by Atomic Layer Deposition,” ECS Transactions, 45(6) 55-67 (2012).
- Kim et al. “A Novel Doping Technology for Ultra-shallow Junction Fabrication: Boron diffusion from Boron-adsorbed Layer by Rapid Thermal Annealing,” Thin Solid Films 369 (2000) 207-212.
- Korean Intellectual Property Office, Office Action for corresponding KR patent application No. 10-2016-0025721, dated Jun. 7, 2017, 2 pages.