Systems and methods for reducing corrosion in a reactor system using fluid encasement
Abstract
Systems and methods for reducing or eliminating corrosion of components of a reactor system, including a supercritical water gasification system, are described. The reactor system may include a reactor vessel configured to receive a reactor fluid through a reactor fluid inlet and a product source fluid corrosive to portions of the reactor system through a product source fluid inlet. The product source fluid may react with the reactor fluid to produce one or more reaction products, such as a fuel gas. The product source fluid inlet may be arranged within the reactor fluid inlet such that the product source fluid entering the reactor vessel is encased by a fluid conduit formed by the flow of reactor fluid entering the reactor vessel. The layer may operate to reduce corrosion by forming a barrier between the product source fluid and the surface of the reactor fluid inlet and/or the reactor vessel.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A reactor system configured to reduce corrosion of portions thereof, the reactor system comprising: at least one reactor vessel comprising an inner surface, at least one reactor fluid inlet, and at least one product source fluid inlet, wherein the at least one reactor fluid inlet is configured to provide reactor fluid into the at least one reactor vessel, and wherein the at least one product source fluid inlet is configured to provide product source fluid into the at least one reactor vessel; and at least one product outlet configured to provide a discharge path for the reactor fluid and react
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 12,318,765 B2 | Apparatus for supercritical water gasification | 2025 | 0 |
References Cited — Backward Prior Art (21)
Non-Patent Literature (5)
- Hong, G.T., and Spritzer, M.H., "Supercritical Water Partial Oxidation," Proceedings of the 2002 U.S. DOE Hydrogen Program Review NREL/CP-610-32405, pp. 1-18 (2002).
- International Search Report and Written Opinion for International Patent Application No. PCT/US2013/51613 dated Dec. 23, 2013.
- Kritzer, P., "Corrosion in high-temperature and supercritical water and aqueous solutions: a review," The Journal of Supercritical Fluids, vol. 29, No. 1-2, pp. 1-29 (Apr. 2004).
- Leusbrock, I., "Supercritical Fluids," Removal of Inorganic Compounds via Supercritical Water: Fundamentals and Applications, Chapter 2, Thesis, pp. 39-55 (2011).
- Marrone, P.A., and Hong, G.T., "Corrosion control methods in supercritical water oxidation and gasification processes," The Journal of Supercritical Fluids, vol. 51, No. 2, pp. 83-103 (Dec. 2009).