Resin composition, layered product, multilayer printed wiring board, multilayer flexible wiring board and manufacturing method of the same
Abstract
A resin composition containing (A) a polyimide having acidic functional groups and (B) a compound having functional groups that react with the acidic functional groups, where (a) a solution rate in 3 mass % aqueous sodium hydroxide at 45° C. is 0.95 or more after a heat history of 90° C. for 10 minutes with the solution rate before the heat history assumed to be 1, (b) the solution rate in 3 mass % aqueous sodium hydroxide at 45° C. ranges from 0.001 μm/sec to 0.02 μm/sec after the heat history of 180° C. for 60 minutes, (c) a bleed-out amount is 50 mg/m 2 or less in storing at 40° C. for 2 weeks after the heat history of 180° C. for 60 minutes, and (d) a thermogravimetric decrease at 260° C. is 2.0% or less in measuring on a temperature rising condition of 10° C./min from 40° C. by thermogravimetric analysis (TG). When a multilayer flexible wiring board is manufactured using the resin composition, it is possible to obtain the resin layer excellent in alkali processability, embeddability in press, heat resistance, bendability, insulation reliability, and adhesion to the conductive layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A resin composition containing: (A) a polyimide having acidic functional groups; and (B) a compound having functional groups that react with the acidic functional groups, wherein (a) a solution rate of the resin composition in 3 mass % aqueous sodium hydroxide at 45° C. is 0.95 or more after a heat history of 90° C. for 10 minutes with the solution rate before the heat history assumed to be 1, wherein (b) the solution rate of the resin composition in 3 mass % aqueous sodium hydroxide at 45° C. ranges from 0.001 μm/sec to 0.02 μm/sec after a heat history of 180° C. for 60 minutes, wherein (c) a
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (30)
Non-Patent Literature (2)
- International Preliminary Report on Patentability and English translation of Written Opinion dated Jul. 31, 2014, in PCT International Application No. PCT/JP2013/050978.
- International Search Report issued in PCT/JP2013/050978, dated Apr. 23, 2013.