Abstract

The invention relates to an electrolytic copper alloy foil having large mechanical strength in an ordinary state and showing resistant to heat deterioration even when it is heated to 300° C. or more. That electrolytic copper alloy foil, which contains tungsten copper, preferably incorporates tungsten into copper foil as a copper alloy, has a tensile strength at ordinary temperature of 650 MPa, has a tensile strength after heat treatment at 300° C. for 1 hour of 450 MPa or more, and has a conductivity of 80% or more. Further preferably, the electrolytic copper foil has an elongation at ordinary temperature of 2.5% or more and an elongation after treatment at 300° C. for 1 hour of 3.5% or more. The electrolytic copper foil is produced by adding a thiourea compound, tungsten salt, and chloride ions to a sulfuric acid-copper sulfate electrolyte and performing electrolytic deposition.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (3 — 3 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An electrolytic copper alloy foil comprising from 0.0001 to 0.060 wt % of tungsten, wherein the tungsten is at least partially incorporated as an oxide.

  2. Claim 2Independent Claim

    An electrolytic copper alloy foil, comprising from 0.001 to 0.055 wt % of tungsten, wherein the electrolytic copper alloy foil has a tensile strength at ordinary temperature of 650 MPa or more and a tensile strength after treatment at 300° C. for 1 hour of 450 MPa or more.

  3. Claim 3Independent Claim

    An electrolytic copper alloy foil, comprising from 0.001 to 0.055 wt % of tungsten, wherein the electrolytic copper alloy foil has a tensile strength at ordinary temperature of 650 MPa or more and a tensile strength after treatment at 300° C. for 1 hour of 450 MPa or more, and wherein the electrolytic copper alloy foil has an elongation at ordinary temperature of 2.5% or m

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
JP H03263430 APolysiloxane and production thereof—2
JP H07278867 AProduction of electrolytic copper foil—20
JP H0967693 AProduction of electrolytic copper foil—28
US 2001014408 A1Surface -treated copper foil, method of producing the surface-treated copper foil, and copper-clad laminate employing the surface-treated copper foil—3
KR 20010108414 ASurface treated copper foil and Method for preparing the same and Copper-clad laminate using the same—2
JP 3,238,278 B2電解銅箔の製造方法200112
JP 3,263,430 B2リチウム二次電池20022
JP 3,270,637 B2電着銅箔およびその製造方法20024
CN 1,348,326 AProduction method of copper foil for fine line use—11
US 2002053517 A1Method of producing copper foil for fine wiring—15
TW 499,508 BRoughening treated copper foil and producing method therefor20021
US 6,440,503 B1Laser deposition of elements onto medical devices200241
CN 1,382,310 AElectrode for lithium battery and rechargeable lithium battery—9
US 2002177044 A1Electrode for lithium secondary battery and method for producing the same—41
US 2002182344 A1Laser deposition of elements onto medical devices—7
US 6,497,806 B1Method of producing a roughening-treated copper foil200217
US 6,527,939 B1Method of producing copper foil with an anode having multiple coating layers200332
TW 200,302,036 AElectrodeposited copper foil with carrer foil and method for manufacturing the same and copper-clad laminate using the electrodeposited copper foil with carrier foil—2
US 6,685,804 B1Method for fabricating electrode for rechargeable lithium battery2004110
TW 200,407,465 AElectrolyte solution for manufacturing electrolytic copper foil and electrolytic copper foil manufacturing method using the same—1
US 2004104117 A1Electrolyte solution for manufacturing electrolytic copper foil and electrolytic copper foil manufacturing method using the same—25
US 2004154930 A1Copper foil for high frequency circuit and method of production of same—9
US 2004157080 A1Copper foil for fine pattern printed circuits and method of production of same—25
US 2004157121 A1Electrochemical cell—42
EP 1,448,036 A1Copper foil for fine pattern printed circuits and method of production same—5
CN 1,530,469 AHigh efficient copper foil and producing method thereof—10
US 6,887,511 B1Method for preparing electrode material for lithium battery2005113
CN 1,657,279 ATreated copper foil and circuit board—53
US 6,984,453 B2Electrolyte copper foil having carrier foil, manufacturing method thereof, and layered plate using the electrolyte copper foil having carrier foil20066
US 7,192,673 B1Electrode for rechargeable lithium battery and rechargeable lithium battery2007163

Non-Patent Literature (5)

  • Chin an Huang et al., "Electrocrystallization Behavior of Copper Electrodeposited from Aqueous Sulfuric Acid with Thiourea and Chloride Additives", ECS Transactions, vol. 2, May 7, 2006, XP055196699, pp. 329-334.
  • International Search Report dated Oct. 30, 2012 in PCT/JP2012/069368 filed Jul. 30, 2012.
  • Office Action dated Apr. 16, 2013 in Japanese Patent Application No. 2012-249946 (English translation only).
  • Office Action dated Feb. 28, 2015 in Chinese Patent Application No. 201280004436.7 (English translation only).
  • Office Action dated Jan. 28, 2015 in Korean Patent Application No. 10-2013-7006252 (with English language translation).