Patents
US 9,890,437 B2#82671472 Most CitedActiveUnited States (USPTO)Utility

High-strength steel sheet with excellent warm formability and process for manufacturing same

0Forward Citations (#82671472 Global)
0.0/yrCitation Velocity (#82671472 Global)
0.56Citation PageRank (#82671472 Global)
34Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

This high-strength steel sheet contains, in mass %, 0.05 to 0.3% of C, 1 to 3% of Si, 0.5 to 3% of Mn, up to 0.1% (inclusive of 0%) of P, up to 0.01% (inclusive of 0%) of S, 0.001 to 0.1% of Al and 0.002 to 0.03% of N with the balance consisting of iron and unavoidable impurities, and has a microstructure which comprises, in area fraction relative to the microstructure, 40 to 85% of bainitic ferrite, 5 to 20% of retained austenite (γ R ), 10 to 50% (in total) of martensite and γ R , and 5 to 40% of ferrite. The retained austenite (γ R ) has a C concentration of 0.5 to 1.0 mass %, while the quantity of γ R present in the ferrite grains is 1% or more (in area fraction) relative to the microstructure.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 34 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A steel sheet, comprising: C: from 0.05 mass % to 0.3 mass %; Si: from 1 mass % to 3 mass %; Mn: from 0.5 mass % to 3 mass %; P: from 0 mass % to 0.1 mass %; S: from 0 mass % to 0.01 mass %; Al: from 0.001 mass % to 0.1 mass %; and N: from 0.002 mass % to 0.03 mass %, the balance being iron and impurities; wherein the steel sheet has a microstructure which comprises, in terms of an area fraction relative to the total microstructure area: bainitic.ferrite: from 40 to 85%, retained austenite: from 5 to 20%, martensite and retained austenite: from 10 to 50%, and ferrite: from 9 to 40%, the retain

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (34)

PatentTitleYearCitations
JP 2003113442 AHigh-tensile steel sheet superior in warm forming property—26
US 2005150580 A1Ultra-high strength steel sheet having excellent hydrogen embrittlement resistance, and method for manufacturing the same—55
JP 2006274418 AHigh-strength cold-rolled steel sheet having superior in uniform elongation and manufacturing method therefor—22
WO 2006/109489 A1High-strength cold-rolled steel sheet excellent in coating adhesion, workability and hydrogen embrittlement resistance, and steel component for automobile—5
KR 20070107179 AHigh-strength cold-rolled steel sheet excellent in coating adhesion, workability and hydrogen embrittlement resistance, and steel component for automobile—6
EP 1,865,085 A1High-strength cold-rolled steel sheet excellent in coating adhesion, workability and hydrogen embrittlement resistance, and steel component for automobile—45
JP 2007321237 AHigh-strength steel sheet with composite structure having excellent formability and delayed fracture resistance—15
US 2008251160 A1High-Strength Cold-Rolled Steel Sheet Excellent in Uniform Elongation and Method for Manufacturing Same—21
US 7,468,109 B2High strength steel sheet having excellent stretch flangeability20089
US 2009053096 A1High-strength cold-rolled steel sheet excellent in coating adhesion, workability and hydrogen embrittlement resistance, and steel component for automobile—33
US 7,591,977 B2High strength and low yield ratio cold rolled steel sheet and method of manufacturing the same200914
US 2009242085 A1Dual phase steel sheet with good bake-hardening properties—14
US 2009277547 A1High-strength steel sheets and processes for production of the same—39
JP 4,506,476 B2温間成形に適した冷延鋼板およびその製造方法20102
US 7,767,036 B2High strength cold rolled steel sheet and plated steel sheet excellent in the balance of strength and workability201014
US 2010221138 A1High-strength composite steel sheet having excellent moldability and delayed fracture resistance—28
US 7,887,648 B2Ultrahigh-strength thin steel sheet201111
WO 2011/111333 A1High-strength pressed member and method for producing same—34
JP 2011184758 AHigh strength pressed member and method for producing the same—53
WO 2011/118597 A1High-strength steel plate with excellent warm workability—6
US 2012009434 A1Cold-rolled steel sheet—45
US 2012012231 A1Cold-rolled steel sheet and method for producing the same—23
US 8,197,617 B2High-strength steel sheet having excellent elongation, stretch flangeability and weldability20128
US 8,343,288 B2Cold rolled steel sheet201315
EP 2,546,375 A1High-strength pressed member and method for producing same—37
US 2013022490 A1High-strength steel sheet with excellent warm workability—5
US 2013048161 A1High strength press-formed member and method for manufacturing the same—35
US 2013236350 A1Highly formable high-strength steel sheet, warm working method, and warm-worked automobile part—9
US 2013259734 A1Highly formable high-strength steel sheet, warm working method, and warm-worked automobile part—6
US 8,597,439 B2High-strength cold rolled steel sheet having excellent formability, and plated steel sheet20136

Non-Patent Literature (5)

  • Cai-nian Jing, et al. "Research Progress of the Influencing Factors on Transformation Induced Plasticity" Heat Treatment of Metals, Feb. 2005, Feb. 30, 2005, pp. 26-31 (with English Abstract).
  • Extended European Search Report dated Oct. 1, 2015 in European Patent Application No. 13755142.0.
  • International Search Report dated Apr. 23, 2013, in PCT/JP13/052729 filed Feb. 6, 2013.
  • U.S. Appl. No. 14/238,599, filed Jun. 5, 2014, Murakami, et al.
  • Written Opinion of the International Searching Authority dated Apr. 23, 2013, in PCT/JP13/052729 filed Feb. 6, 2013.