Patents
US 9,890,079 B2#43551947 Most CitedActiveUnited States (USPTO)Utility

Cementitious binders containing pozzolanic materials

2Forward Citations (#43551947 Global)
0.2/yrCitation Velocity (#29288717 Global)
0.93Citation PageRank (#46151268 Global)
18Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A cementitious composition including: a binder containing (a) 60-94%, by weight, of at least one pozzolanic material; (b) at least 0.5% calcium sulfoaluminate (CSA), by weight; (c) 1.2-11% by weight, expressed as SO 3 , of at least one inorganic sulfate selected from the group of sulfates consisting of a calcium sulfate hemihydrate, an anhydrous calcium sulfate, a calcium sulfate dihydrate, a sodium sulfate, and a sodium calcium sulfate; and (d) a total sulfate content of at least 3%, by weight, expressed as SO 3 , the cementitious composition including, at most, 3% natural lime, the cementitious composition including, at most, 10% alumina cement, the contents of the composition being calculated on a dry, aggregateless basis.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A cementitious composition comprising: a binder containing: (a) 72-94%, by weight, of ground granular blast furnace slag (GGBFS); (b) at least 0.5% calcium sulfoaluminate (CSA), by weight, said CSA having the structure 3CaO.3Al 2 O 3 .CaSO 4 ; (c) 1.2-11% by weight, expressed as SO 3 , of at least one inorganic sulfate selected from the group of sulfates consisting of a calcium sulfate hemihydrate, an anhydrous calcium sulfate, a calcium sulfate dihydrate, a sodium sulfate, and a sodium calcium sulfate; and (d) a total sulfate content of at least 3%, and at most 11%, by weight, expressed as SO

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (18)

PatentTitleYearCitations
GB 513,898 AImprovements in and relating to the manufacture of cements from calcium sulphate and blast furnace slag—7
GB 2,099,808 AHydraulic cement—11
US 4,404,031 AProcess for producing hydraulic cements198326
JP H02217346 ALining material and production of lined pipe using same material—10
EP 0,727,398 A2Composite cement—3
CN 1,172,084 ANon-chamotte burning-free flyash cement—16
KR 20000044702 AProduction method of fly-ash mixing mortar to increase early strength—5
KR 20020049817 AThe method for manufacturing of soil stability for treatment—7
KR 20030005733 AThe composition of ceramic coating material having function—12
KR 100,592,781 B1Water-permeable concrete composition using bottom ash200614
US 2007266903 A1High Belite-Containing Sulfoaluminous Clinker, Method for the Production and the Use Thereof for Preparing Hydraulic Binders—37
KR 20090032729 AManufacturing method for soil blocks to be used for environmetal artificial fish selters—10
KR 100,896,005 B1Admixture composite for strength improvement of ready-mixed concrete and concrete production method using the same20098
RU 2,360,874 C2Sulphoaluminate clinker with high belite content, method for its preparation and its application for hydraulic binders20093
KR 100,931,008 B1Water-permeable paving materials using environmentally friendly inorganic binders and its constructing method thereof200915
KR 20100002234 AHydrophile property aerogel powders—17
FR 2,949,112 A1Additifs pour liant hydraulique a base de clinker belite - calcium - sulphoalumineux - ferrite (bcsaf)—15
US 2012145045 A1Additives for a hydraulic binder based on belite-calcium-sulphoaluminate-ferrite clinker—11

Non-Patent Literature (2)

  • M. Michel et al., "The influence of gypsum ratio on the mechanical performance of slag cement accelerated by calcium sulfoaluminate cement", Construction and Building Materials, vol. 25, pp. 1298-1304 (2011)).
  • Takuma et al., "Hydration and pH Behavior of the Cement Prepared from the Mixture of Hauyne-Containing Clinker, Anhydrite and Blastfurnace Slag", Journal of the Ceramic Society of Japan, Int. Edition, vol. 104, pp. 1044-1052, 1996.