Patents
US 9,873,629 B2#61326616 Most CitedActiveUnited States (USPTO)Utility

Methods for producing optical fiber preforms with low index trenches

1Forward Citations (#61326616 Global)
0.1/yrCitation Velocity (#42665598 Global)
0.75Citation PageRank (#61326616 Global)
30Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Methods for forming optical fiber preforms with low-index trenches are disclosed. According to one embodiment, the method includes depositing silica-based glass soot on a bait rod to form a low-index trench region of the optical fiber preform. The silica-based glass soot is deposited such that the low-index trench region has a first density. Thereafter a barrier layer having a second density greater than the first density is formed around the low-index trench region. Therafter, an overclad region is deposited around the barrier layer. The bait rod is then removed from a central channel of the trench-overclad assembly. A separate core assembly is inserted into the central channel. A down-dopant gas is then directed through the central channel of the trench-overclad assembly as the trench-overclad assembly is heated to dope the low-index trench region. The barrier layer prevents diffusion of the down-dopant from the low-index trench region into the overclad region.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for forming an optical fiber preform, the method comprising: depositing silica glass on a bait rod thereby forming a trench region, wherein the silica glass is deposited such that the trench region has a first density, said first density being less than 0.6 g/cm 3 ; forming a barrier layer of silica glass around the trench region, wherein the barrier layer of silica glass has a second density that is greater than the first density, said second density being at least 1.75 g/cm 3 ; depositing silica glass around the barrier layer with the second density thereby forming an overclad regio

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (30)

PatentTitleYearCitations
US 3,932,162 AMethod of making glass optical waveguide197698
GB 1,456,371 AOptical transmission fibre—10
US 4,518,407 AOptical fibre preform manufacture19857
US 4,620,861 AMethod for making index-profiled optical device198656
US 4,627,867 AMethod for producing highly pure glass preform for optical fiber198628
US 4,629,485 AMethod of making fluorine doped optical preform and fiber and resultant articles1986100
US 4,648,891 AOptical fiber198713
US 4,668,263 AMethod for producing glass preform for optical fiber198762
US 4,749,396 AMethod of forming an optical fiber preform198824
US 4,772,302 AOptical waveguide manufacture198836
US 4,834,786 AMethod of manufacturing a preform for asymmetrical optical fiber198921
US 5,000,773 AProcess for producing preforms for optical fibers199112
US 5,342,597 AProcess for uniformly moisturizing fumed silica199455
US 5,641,333 AIncreasing the retention of Ge02 during production of glass articles19974
WO 9,833,746 A1Method of having optical fiber having depressed index core region—11
US 5,917,109 AMethod of making optical fiber having depressed index core region199984
US 6,189,342 B1Method of making segmented core optical waveguide preforms200121
US 2003046960 A1Single step laydown method of making dry fiber with complex fluorine doped profile—15
US 2003200771 A1Method of manufacturing phosphosilicate optical fibers and optical fibers formed therefrom—3
US 6,690,868 B2Optical waveguide article including a fluorine-containing zone200422
US 6,883,351 B2Method for fabricating a low polarization mode dispersion optical fiber20056
US 6,928,841 B2Optical fiber preform manufacture using improved VAD20056
US 7,058,269 B2Reconstructed glass for fiber optic applications20066
US 7,089,766 B2Method of forming optical fiber preforms20067
US 2008013901 A1Macro-bending insensitive optical fiber—7
US 2008260339 A1Manufacture of depressed index optical fibers—7
US 2009169163 A1Bend Resistant Multimode Optical Fiber—176
US 7,603,015 B2Optical fiber with large effective area200926
US 7,620,282 B2Low bend loss single mode optical fiber200930

Non-Patent Literature (2)

  • Chinese First Office Action 201280031881.2 dated May 26, 2015.