Patents
US 9,857,487 B2#37802678 Most CitedActiveUnited States (USPTO)Utility

Solid marine seismic streamers

2Forward Citations (#37802678 Global)
0.2/yrCitation Velocity (#28813744 Global)
1.09Citation PageRank (#37207995 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A marine seismic streamer comprising a solid, hydrophobic core member that is encased in a hydrophobic streamer skin/casing. The hydrophobic streamer skin may be extruded onto and/or heat welded to the hydrophobic core member. The hydrophobic streamer skin/casing may comprise a thermoplastic polyurethane that includes fluorine and/or silicon moieties, silicon, polydimethylsiloxane or the like. The hydrophobic streamer skin/casing may reduce the drag of the streamer and may provide anti-biofouling properties to the streamer. A hydrophobic paint, coating or polymer may in some instances be disposed on top of the hydrophobic streamer skin/casing.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A seismic streamer, comprising: a streamer body comprising a solid, hydrophobic material that includes silicon or fluorine moieties; and a streamer casing distinct from the streamer body, the streamer casing including a sleeve that encases the streamer body, and the streamer casing comprising a hydrophobic material.

  2. Claim 2Depends on #1

    The seismic streamer of claim 1 , wherein the streamer body defines a cylinder with a hollow core.

  3. Claim 3Depends on #1

    The seismic streamer of claim 1 , wherein the streamer body includes a material selected from the group consisting of polyethylene, polypropylene, polytetrafluoroethylene and thermoplastic polyurethane.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,064,338 AMethod for preparing biologically active copolymers of triorganotin acrylates197713
JP S6424823 APolyurethane emulsion—6
JP S6445878 APorous sheet material and production thereof—2
US 5,331,074 AAntifouling coating compositions199446
US 5,449,553 ANontoxic antifouling systems199550
US 5,514,731 AAntifouling paint199624
JP H0912413 AAquatic antifouling agent—6
US 5,637,772 AFluorinated diamines and polymers formed therefrom199765
JP H09183199 ALaminated film—5
US 5,691,019 AFoul release system199728
KR 0,159,478 B1Polyolefin anti-fouling resin composition19985
US 5,904,988 ASprayable, condensation curable silicone foul release coatings and articles coated therewith199933
US 5,906,893 ASprayable, addition curable silicone foul release coatings and articles coated therewith199913
WO 9,926,992 A1Room temperature curable silane terminated and stable waterborne polyurethane dispersions which contain fluorine and/or silicone and low surface energy coatings prepared therefrom—28
US 6,020,026 AProcess for the production of a coating of molecular thickness on a substrate200023
US 6,048,580 AFouling release coating for marine vessels and method of application200016
US 6,101,973 AApparatus for reducing friction on polymeric surfaces200025
US 6,221,498 B1Antifouling silicone emulsion coating-composition, process for producing the same and antifouling article coated therewith200142
US 2001032568 A1Silane-based, coating compositions, coated articles obtained therefrom and methods of using same—76
US 2001034413 A1Fluorine-containing diols and use thereof—6
US 6,313,335 B1Room temperature curable silane terminated and stable waterborne polyurethane dispersions which contain fluorine and/or silicone and low surface energy coatings prepared therefrom200188
US 2001051274 A1Antifouling compounds and uses thereof—10
US 6,403,105 B1Curable silicone foul release coating and articles200236
CN 1,661,731 ALongitudinal watertightness cable/wire—42
US 2005255251 A1Composition, method of making, and treatment of wood with an injectable wood preservative slurry having biocidal particles—77
US 2006002234 A1Anti-biofouling seismic streamer casing and method of manufacture—23
WO 2006/005045 A2Anti-biofouling seismic streamer casing and method of manufacture—6
US 2006022020 A1Method for the production of a metal-ceramic substrate, preferably a copper ceramic substrate—7

Non-Patent Literature (5)

  • Brady, et al., “Mechanical Factors Favoring Release From Fouling Release Coatings,” Biofouling, vol. 15, Issues 1-3, 2000, pp. 73-81. (Provided under U.S. Appl. No. 13/553,588).
  • Chattopadhyay, Dipak Kumar, and K. V. S. N. Raju. “Structural engineering of polyurethane coatings for high performance applications.” Progress in polymer science 32.3 (2007): 352-418.
  • Chunfeng Ma, Yi Hou, Shi Liu, and Guangzhao Zhang, “Effect of Microphase Separation on the Protein Resistance of a Polymeric Surface”, Langmuir 2009, 25 (16), 9467-9472. (Provided under U.S. Appl. No. 13/553,588).
  • Combined Search and Examination Report issued in United Kingdon Application No. 1110087.2, dated Oct. 14, 2011, 20 pages. (Provided under U.S. Appl. No. 13/553,588).