Patents
US 9,834,860 B2#41634704 Most CitedActiveUnited States (USPTO)Utility

Method of high growth rate deposition for group III/V materials

2Forward Citations (#41634704 Global)
0.2/yrCitation Velocity (#31693044 Global)
0.97Citation PageRank (#43212666 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Embodiments of the invention generally relate processes for epitaxial growing Group III/V materials at high growth rates, such as about 30 μm/hr or greater, for example, about 40 μm/hr, about 50 μm/hr, about 55 μm/hr, about 60 μm/hr, or greater. The deposited Group III/V materials or films may be utilized in solar, semiconductor, or other electronic device applications. In some embodiments, the Group III/V materials may be formed or grown on a sacrificial layer disposed on or over the support substrate during a vapor deposition process. Subsequently, the Group III/V materials may be removed from the support substrate during an epitaxial lift off (ELO) process. The Group III/V materials are thin films of epitaxially grown layers which contain gallium arsenide, gallium aluminum arsenide, gallium indium arsenide, gallium indium arsenide nitride, gallium aluminum indium phosphide, phosphides thereof, nitrides thereof, derivatives thereof, alloys thereof, or combinations thereof.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for forming a gallium arsenide material on a wafer, comprising: heating a wafer to a deposition temperature of greater than 650 C and less than 750 C within a processing system; exposing the wafer to a deposition gas comprising a gallium precursor gas and arsine at a total pressure of greater than 50 Torr and less than 450 Torr; and depositing one or more gallium arsenide layers on the wafer at a deposition rate selected from the group consisting of a 30 μm/hr deposition rate, a 40 μm/hr deposition rate, a 50 μm/hr deposition rate, a 55 μm/hr deposition rate, and a 60 μm/hr deposition

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,993,533 AMethod for making semiconductors for solar cells1976113
US 4,172,756 AMethod for the accelerated growth from the gaseous phase of crystals, and products obtained in this manner197910
US 4,368,098 AEpitaxial composite and method of making198385
US 4,445,965 AMethod for making thin film cadmium telluride and related semiconductors for solar cells198481
US 4,727,047 AMethod of producing sheets of crystalline material1988446
US 4,846,931 AMethod for lifting-off epitaxial films1989211
US 4,878,989 AChemical beam epitaxy system198928
US 4,883,561 ALift-off and subsequent bonding of epitaxial films1989221
US 5,073,230 AMeans and methods of lifting and relocating an epitaxial device layer1991200
US 5,076,860 AAlgan compound semiconductor material199187
US 5,122,852 AGrafted-crystal-film integrated optics and optoelectronic devices199272
US 5,168,077 AMethod of manufacturing a p-type compound semiconductor thin film containing a iii-group element and a v-group element by metal organics chemical vapor deposition199239
US 5,201,996 APatterning method for epitaxial lift-off processing199350
US 5,221,637 AMesa release and deposition (MRD) method for stress relief in heteroepitaxially grown GaAs on Si199331
US 5,232,869 AMetal deposition199328
US 5,256,562 AMethod for manufacturing a semiconductor device using a circuit transfer film1993166
US 5,258,325 AMethod for manufacturing a semiconductor device using a circuit transfer film1993261
US 5,276,345 AComposite GaAs-on-quartz substrate for integration of millimeter-wave passive and active device circuitry199445
US 5,277,749 AMethods and apparatus for relieving stress and resisting stencil delamination when performing lift-off processes that utilize high stress metals and/or multiple evaporation steps1994112
US 5,286,335 AProcesses for lift-off and deposition of thin film materials1994110
US 5,344,517 AMethod for lift-off of epitaxial layers and applications thereof199470
US 5,401,983 AProcesses for lift-off of thin film materials or devices for fabricating three dimensional integrated circuits, optical detectors, and micromechanical devices1995316
US 5,402,748 AMethod of growing a compound semiconductor film199528
US 5,458,694 AMultispectral photovoltaic component comprising a stack of cells, and method of manufacture1995101
US 5,465,009 AProcesses and apparatus for lift-off and bonding of materials and devices1995127
US 5,476,810 AManufacture of electronic devices comprising thin-film circuits using a metal foil as a temporary support199559
US 5,479,043 AMultispectral photovoltaic component199565
US 5,528,719 AOptical fiber guide structure and method of fabricating same199663

Non-Patent Literature (5)

  • Bauhuis, G.J., "Substrate Reuse for Epitaxial Lift-Off of III-V Solar Cells", Proceedings of the 22nd European Photovoltaic Solar Energy Conference: Milan Sep. 3-7, 2007, pp. 106-110.
  • Bauhuis, G.J., "Thin film GaAs solar cells with increased quantum efficiency due to light reflection", Solar Energy Materials & Solar Cells 83 (2004) 81-90, Nov. 3, 2003.
  • Konagai, Makoto, "High Efficiency GaAs Thin Film Solar Cells by Peeled Film Technology", Journal of Crystal Growth 45 (1978) 277-280.
  • Kumar; P., "Sacrificial etching of AlxGa1-xAs for III-V MEMS surface micromachining", Appl. Phys. A 88, 711-714, May 24, 2007.
  • Schermer J.J., "Epitaxial Lift-Off for large area thin film III/V devices", Phys. Stat. Sol. (1) 202, No. 4, 501-508 (2005).