US 9,828,286 B2#18927126 Most CitedActiveUnited States (USPTO)Utility

Method for producing chemically strengthened glass

6Forward Citations (#18927126 Global)
0.7/yrCitation Velocity (#11792015 Global)
1.15Citation PageRank (#34190445 Global)
45Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method for producing a chemically strengthened glass, including a step of bringing a glass containing sodium into contact with an inorganic salt containing potassium nitrate, thereby performing ion exchange of a Na ion in the glass with a K ion in the inorganic salt, in which the inorganic salt contains at least one salt selected from the group consisting of K 2 CO 3 , Na 2 CO 3 , KHCO 3 , NaHCO 3 , K 3 PO 4 , Na 3 PO 4 , K 2 SO 4 , Na 2 SO 4 , KOH and NaOH, and the method includes: a step of washing the glass after the ion exchange; a step of subjecting the glass to an acid treatment after the washing; and a step of subjecting the glass to an alkali treatment after the acid treatment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 45 · Forward citations: 6.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for producing a chemically strengthened glass, comprising: bringing a glass comprising sodium into contact with an inorganic salt comprising potassium nitrate, thereby performing ion exchange of a Na ion in the glass with a K ion in the inorganic salt; washing the glass after the ion exchange; bringing the glass into contact with an acid after the washing such that a low-density layer is formed in a surface portion of the glass; and bringing the glass into contact with an alkali after contacting the acid such that at least part of the low-density layer is removed, wherein the inorgani

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the i

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (45)

PatentTitleYearCitations
JP 2001002451 AGlass substrate and its production—21
JP 2002150547 AMethod for manufacturing glass substrate for information recording medium—25
US 2002121110 A1Method of manufacturing glass substrate for information recording media and glass substrate manufactured using the method—31
US 2003079500 A1Method for manufacturing information recording medium glass substrate—27
US 2003164005 A1Method for manufacturing glass substrate of information recording medium—38
US 2003230552 A1PH adjustment of a melt for use in microetching glass substrates—8
US 2004221615 A1Method and apparatus for strengthening glass—52
US 7,140,203 B2Method for manufacturing glass substrate of information recording medium200615
WO 2008/062662 A1Method for producing glass substrate for information recording medium, glass substrate for information recording medium, and information recording medium—11
JP 2008195602 AMethod for manufacturing tempered glass substrate and tempered glass substrate—99
US 2009197048 A1Damage resistant glass article for use as a cover plate in electronic devices—201
JP 2010108592 AGlass substrate for magnetic disk, and magnetic disk—30
US 2010167059 A1Glass substrate and method for manufacturing the same—31
JP 2010168270 AGlass substrate and method for manufacturing the same—30
JP 2011510904 A電子装置のカバープレートとして使用するための耐損傷性ガラス物品—63
US 2011165393 A1Impact-damage-resistant glass sheet—109
US 2011171415 A1Glass substrate for a magnetic disk and magnetic disk—23
CN 102,432,171 AGlass for use as substrate for information recording medium and chemical reinforcing glass—11
CN 102,583,966 ACover glass for flat panel displays—4
US 2012208028 A1Glass substrate and method for manufactring the same—8
JP 2012236737 AGlass manufacturing method, and glass—17
JP 2012250861 AChemically strengthened glass plate—27
JP 2013040086 AMethod for manufacturing tempered glass plate and cover glass, and cover glass—11
WO 2013/035840 A1Process for producing cover glass for potable appliance—12

Non-Patent Literature (5)

  • International Search Report dated Oct. 21, 2014 in PCT/JP2014/068832, filed Jul. 15, 2014 (with English Translation).
  • International Search Report dated Oct. 21, 2014 in PCT/JP2014/068834, filed Jul. 15, 2014 (with English Translation).
  • International Search Report dated Oct. 21, 2014 in PCT/JP2014/068836, filed Jul. 15, 2014 (with English Translation).
  • S. Ito et al. "Crack Blunting of High-Silica Glass", Journal of the American Ceramic Society, vol. 65, No. 8, 1982, 2 pages.
  • Won-Taek Han et al. "Effect of Residual Water in Silica Glass on Static Fatigue", Journal of Non-Crystalline Solids, vol. 127, 1991, 5 pages.