Patents
US 9,815,147 B2#60607223 Most CitedActiveUnited States (USPTO)Utility

High strength Ni—Cr—Mo—W—Nb—Ti welding product and method of welding and weld deposit using the same

1Forward Citations (#60607223 Global)
0.1/yrCitation Velocity (#44851105 Global)
0.76Citation PageRank (#60607223 Global)
48Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A welding filler metal or a welding filler metal product having, in weight percent: 17.0-23.0% chromium, 5.0-12.0% molybdenum, 3.0-11.0% tungsten, 3.0-5.0% niobium, 0-2.0% tantalum, 1.2-3.0% titanium, 0.005-1.50% aluminum, 0.0005-0.100% carbon, <2.0% iron, <5.0% cobalt, and balance nickel wherein the nickel is 56.0-65.0%. A weld deposit formed from the welding filler metal has a minimum yield strength in the as-welded condition of at least 72 ksi (496 MPa). Also, a weld deposit and a method of forming a weld deposit comprising, in weight percent: 17.0-23.0% chromium, 5.0-12.0% molybdenum, 3.0-11.0% tungsten, 3.0-5.0% niobium, 0-2.0% tantalum, 1.2-3.0% titanium, 0.005-1.50% aluminum, 0.0005-0.100% carbon, <8.0% iron, <5.0% cobalt, and balance nickel wherein the nickel is 56.0-65.0%. The weld deposit has a minimum yield strength in the as-welded condition of at least 72 ksi (496 MPa).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 48 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A welding filler metal comprising, in weight percent: 17.0 to 23.0% chromium, 5.0 to 12.0% molybdenum, 3.0 to 11.0% tungsten, 3.0 to 5.0% niobium, 0 to 2.0% tantalum, 1.2 to 3.0% titanium, 0.005 to 1.50% aluminum, 0.0005 to 0.100% carbon, less than 2.0% iron, less than 5.0% cobalt, and balance nickel wherein the nickel is 56.0 to 65.0%, and wherein a weld deposit formed from the welding filler metal has a minimum yield strength in an as-welded condition of at least 72 ksi (496 MPa).

  2. Claim 2Depends on #1

    The welding filler metal of claim 1 comprising a minimum of 3.5% niobium+tantalum.

  3. Claim 3Depends on #1

    The welding filler metal of claim 1 comprising a maximum of 6.0% niobium+tantalum.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (48)

PatentTitleYearCitations
US 2,400,255 AElectric resistance elements and the like194613
GB 974,185 AA method of producing chromium diffusion zones—6
US 3,311,972 AProduction of ingots for wrought metal products19676
US 3,479,157 AWelded articles and alloys containing hafnium and nickel196922
US 3,512,963 AProcess for improving elevated temperature strength and ductility of nickel-base alloys197012
US 3,632,319 ADiffusion bonding of superalloy members197263
US 3,785,877 ATreating nickel base alloys197444
US 3,865,581 AHeat resistant alloy having excellent hot workabilities197594
US 3,865,575 AThermoplastic prealloyed powder197514
US 4,359,352 ANickel base superalloys which contain boron and have been processed by a rapid solidification process198232
US 4,409,462 AProcess for the non-cracking energy beam welding of high temperature shaped parts198346
US 4,765,956 ANickel-chromium alloy of improved fatigue strength198855
US 5,328,499 AMechanically alloyed nickel-base composition having improved hot formability characteristics199415
CA 1,336,945 CCorrosion resistant age hardenable nickel-base alloy19951
US 5,556,594 ACorrosion resistant age hardenable nickel-base alloy199674
US 5,725,693 AFiller metal alloy for welding cast nickel aluminide alloys19987
US 6,177,046 B1Superalloys with improved oxidation resistance and weldability200166
US 6,242,113 B1Welding alloy and articles for use in welding, weldments and methods for producing weldments200152
CA 2,392,754 A1Method for the production of a heat resistant alloy with good resistance to high-temerature oxidation—3
US 6,298,817 B1Exhaust valve for an internal combustion engine200131
US 6,302,649 B1Superalloy weld composition and repaired turbine engine component200137
US 6,315,846 B1Heat treatment for nickel-base alloys200151
US 6,354,799 B1Superalloy weld composition and repaired turbine engine component200220
US 6,478,897 B1Heat-resistant alloy wire200235
US 2002166844 A1Room-temperature surface weld repair of nickel-base superalloys having a nil-ductility range—13
US 2003005981 A1Ni-base heat resistant alloy and welded joint thereof—49
US 2004076540 A1Welding material, gas turbine blade or nozzle and a method of repairing a gas turbine blade or nozzle—25
US 2004079453 A1Nickel-base alloy and its use in casting and welding operations—26
JP 2004136301 AWelding material, welded structure, blade of gas turbine, and method for repairing rotary blade or stationary blade of gas turbine—22

Non-Patent Literature (3)

  • 625 Inconel® 625 Alloy Brochure; Special Metals Corporation, Aug. 13, 2013; pp. 1-18.
  • Inco-Weld® 725NDUR Filler Metal Brochure; Ni-Cr-Mo Filler Metal; Special Metals Welding Products Company; www.specialmetalswelding.com; at least as early as Apr. 1, 2014; 1 page.
  • Inco-Weld® 725NDUR Filler Metal Brochure; Ni—Cr—Mo Filler Metal; Special Metals Welding Products Company; www.specialmetalswelding.com; at least as early as Apr. 1, 2014; 1 page.