Patents
US 9,799,513 B2#34081705 Most CitedActiveUnited States (USPTO)Utility

Localized elastic strain relaxed buffer

3Forward Citations (#34081705 Global)
0.3/yrCitation Velocity (#23912443 Global)
0.95Citation PageRank (#44934417 Global)
14Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A strain relaxed buffer layer is fabricated by melting an underlying layer beneath a strained semiconductor layer, which allows the strained semiconductor layer to elastically relax. Upon recrystallization of the underlying layer, crystalline defects are trapped in the underlying layer. Semiconductor layers having different melting points, such as silicon germanium layers having different atomic percentages of germanium, are formed on a semiconductor substrate. An annealing process causes melting of only the silicon germanium layer that has the higher germanium content and therefore the lower melting point. The silicon germanium layer having the lower germanium content is elastically relaxed upon melting of the adjoining silicon germanium layer and can be used as a substrate for growing strained semiconductor layers such as channel layers of field-effect transistors.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A fabrication method comprising: obtaining a structure including a semiconductor substrate layer comprising silicon, a strained epitaxial first layer having the composition Si 1-x Ge x on the substrate layer, and a strained epitaxial second layer in direct contact with the first layer and having the composition Si 1-y Ge y wherein y is less than x; forming recesses extending through the first and second layers; subsequent to forming the recesses, melting the first layer while the substrate layer and the second layer remain in a solid state, thereby causing elastic relaxation of the second la

  2. Claim 2Depends on #1

    The method of claim 1 , wherein x is between 0.3 and 1.0, further including avoiding any plastic relaxation of the second layer during a te

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Chleirigh, C. Ni et al., Laser Spike Annealing of Strained Si/Strained Si0.3Ge0.7/Relaxed Si0.7Ge0.3 Dual Channel High Mobility p-MOSFETs, 2010th ECS Meeting, Abstract #1035.