Patents
US 9,783,452 B2#32072377 Most CitedActiveUnited States (USPTO)Utility

Ion-exchanged glass of high surface compression and shallow depth of layer with high resistance to radial crack formation from vickers indentation

3Forward Citations (#32072377 Global)
0.3/yrCitation Velocity (#23399853 Global)
1.12Citation PageRank (#35707188 Global)
27Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Disclosed are alkali aluminosilicate glasses having unexpected resistance to indentation cracking. The glasses obtain this high resistance as a result of a high level of surface compression accompanied by a shallow depth of layer. The advantaged glasses show greater resistance to radial crack formation from Vickers indentation than glasses with the same compressive stress, but higher depths of layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 27 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    3<[(P 2 O 5 +R 2 O)/M 2 O 3 ]≦2.3,  ii. where M 2 O 3 ═Al 2 O 3 +B 2 O 3 , R x O is the sum of monovalent and divalent cation oxides present in the glass composition, and R 2 O is the sum of monovalent cation oxides present in the glass composition and the glass composition is capable of achieving a compressive stress from about 600 to about 1200 MPa at a depth of layer from about 10 to about 40 μm and

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (27)

PatentTitleYearCitations
US 3,357,876 AMethod of strengthening a glass article by ion exchange1967176
US 6,818,576 B2Glass substrate for information recording medium and magnetic information recording medium to which the glass substrate is applied200471
US 2008286548 A1Down-drawable, chemically strengthened glass for cover plate—161
US 2009197088 A1Tempered glass substrate and method of producing the same—170
US 2010047521 A1Durable glass housings/enclosures for electronic devices—197
US 2011045961 A1Zircon compatible glasses for down draw—124
US 2011294648 A1Ion exchangeable glasses—121
US 8,158,543 B2Fining agents for silicate glasses201296
US 8,187,987 B2Durable glass housings/enclosures for electronic devices201247
US 2012135226 A1Ion exchangable glass with deep compressive layer and high damage threshold—109
US 8,232,218 B2Ion exchanged, fast cooled glasses201253
US 2012196110 A1Tempered glass and tempered glass sheet—71
US 8,327,666 B2Method of separating strengthened glass201217
US 8,341,976 B2Method of separating strengthened glass201317
US 8,367,208 B2Damage resistant chemically-toughened protective cover glass201310
WO 2013/073685 A1Glass for chemical reinforcement and chemically reinforced glass—29
US 8,586,492 B2Crack and scratch resistant glass and enclosures made therefrom201392
US 8,759,238 B2Ion exchangeable glasses201432
US 8,765,262 B2Ion exchangeable glass with high crack initiation threshold201443
US 8,796,165 B2Alkaline earth alumino-borosilicate crack resistant glass201427
US 8,802,581 B2Zircon compatible glasses for down draw201431
US 2014226090 A1Glass for chemical tempering and chemically tempered glass—14
US 2015024210 A1Zircon compatible glasses for down draw—3
US 9,156,724 B2Ion exchangeable glass with high crack initiation threshold201551
US 2015368150 A1Ion exchangeable glass with high crack initiation threshold—5
US 9,290,413 B2Ion exchangeable glass with high compressive stress201623
US 9,556,058 B2Zircon compatible glasses for down draw20173

Non-Patent Literature (5)

  • Arora, D.B. Marshall, and B.R. Lawn, "Indentation deformation/fracture of normal and anomalous glasses," Journal of Non-Crystalline Solids, 31 415-428 (1979).
  • Hagan and M.V. Swain, "The origin of median and lateral cracks around plastic indents in brittle materials," J. Phys. D: Appl. Phys., 11 2091-2102 (1978).
  • Hagan and S. Van Der Zwaag, "Plastic processes in a range of soda-lime-silica glasses," Journal of Non-Crystalline Solids, 64 249-268 (1984).
  • Hagan, "Shear deformation under pyramidal indentations in soda-lime glass," Journal of Materials Science, 15 1417-1424 (1980).
  • Kato et al. "Effect of densification on crack initiation under Vickers indentation test," 356 J. Non-Crystalline Solids 1768-1773 (2010).