PECVD protective layers for semiconductor devices

2Forward Citations (#44936348 Global)
0.2/yrCitation Velocity (#31887069 Global)
0.88Citation PageRank (#48942034 Global)
26Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A semiconductor device includes a plasma-enhanced chemical vapor deposition (PECVD) protective layer configured to prevent failure of the semiconductor device throughout a temperature humidity with bias (THB) test exceeding about 1000 hours and/or a highly accelerated stress test (HAST) exceeding about 96 hours. Including a PECVD protective layer capable of protecting the semiconductor device throughout a THB test exceeding about 1000 hours and/or a HAST exceeding about 96 hours results in an extremely robust device, while providing the protective layer via PECVD results in convenience and cost savings.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A semiconductor device comprising a plasma-enhanced chemical vapor deposition (PECVD) protective layer configured to prevent failure of the semiconductor device throughout a temperature humidity with bias (THB) test exceeding about 1000 hours, wherein the PECVD protective layer comprises alternating layers of silicon nitride (SiN) and silicon-oxy-nitride (SiON).

  2. Claim 2Depends on #1

    The semiconductor device of claim 1 wherein the PECVD protective layer is configured to prevent failure of the semiconductor device throughout a THB test exceeding about 1500 hours.

  3. Claim 3Depends on #1

    The semiconductor device of claim 1 wherein the THB test is performed at about 85° C. and about 85% relative humidity.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (26)

PatentTitleYearCitations
US 6,107,096 AMethod of fabricating a salicide-structured MOS semiconductor device having a cobalt disilicied film200016
US 6,211,083 B1Use of a novel capped anneal procedure to improve salicide formation200126
US 6,251,775 B1Self-aligned copper silicide formation for improved adhesion/electromigration200134
KR 20020054845 Amethod for forming of thin film transistor—2
US 6,790,778 B1Method for capping over a copper layer200420
US 2005158957 A1Creating shallow junction transistors—12
US 2006024879 A1Selectively strained MOSFETs to improve drive current—50
US 2006076585 A1Semiconductor resistor and method for manufacturing the same—15
US 2007093013 A1Method for fabricating a gate dielectric of a field effect transistor—28
US 2007123044 A1Method of forming an insulating capping layer for a copper metallization layer by using a silane reaction—28
US 2007243386 A1Process for preparation of multi-thin layered structure—9
US 2007263164 A1Display device and manufacturing method thereof—36
US 2008113521 A1METHOD OF FORMING ULTRA-THIN SiN FILM BY PLASMA CVD—9
US 2008150145 A1Adhesion and electromigration performance at an interface between a dielectric and metal—41
US 2010032643 A1Memory cell that includes a carbon-based memory element and methods of forming the same—19
US 2012056191 A1Semiconductor device, method of manufacturing the same, and power supply apparatus—47
US 2013040163 A1Stainless steel-and-amorphous alloy composite and method for manufacturing—6
US 2013092947 A1Semiconductor device and method of making—21
US 2013092967 A1Led device and method for manufacturing same—2
US 2013200367 A1Semiconductor device—9
US 2014062906 A1Touch screens and methods of manufacturing the same—5
US 2014103360 A1Semiconductor device—7
US 2014151842 A1Semiconductor apparatus—3
US 2014167114 A1Method for Growing III-V Epitaxial Layers—10
US 2016091616 A1Radiation detector and method for manufacturing the same—6
US 2016097123 A1Multiple temperature range susceptor, assembly, reactor and system including the susceptor, and methods of using the same—10

Non-Patent Literature (2)

  • Hussein et al., "Optimization of plasma-enhanced chemical vapor deposition silicon oxynitride layers for integrated optics applications," Thin Solid Films 515 (2007) 3779-3786.
  • Oxford, "Basic PECVD Plasma Processes (SiH4 based)," 2003, http://wcam.engr.wisc.edu/Public/Reference/Deposition/PECVD%20of%20silicon%20nitride%20and%20oxide.pdf.