Method of producing electrical steel sheet
Abstract
A method produces a high strength electrical steel sheet in which a cumulative rolling reduction ratio in rough rolling is 73.0% or more, in which in a hot band annealing step, an annealing condition is selected that satisfies an area ratio of recrystallized grains after hot band annealing of 100%, and a recrystallized grain size of 80 μm to 300 μm, under a condition where annealing temperature is 850° C. to 1000° C., and annealing duration is 10 seconds to 10 minutes, and in which in a final annealing step, an annealing condition is selected that satisfies an area ratio of recrystallized grains after the final annealing of 30% to 95%, and a length in the rolling direction of a connected non-recrystallized grain group of 2.5 mm or less, under a condition where annealing temperature is 670° C. to 800° C., and annealing duration is 2 seconds to 1 minute.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
a
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (28)
Non-Patent Literature (4)
- English translation of the Notification of Reasons for Refusal of corresponding JP 2013-537354 dated Dec. 17, 2013.
- Machine translation of JP-2012136763A (no date available).
- Machine translation of JP-2012136764A (no date available).
- Supplementary European Search Report dated Jul. 22, 2015 of corresponding European Application No. 13752273.6.