Inorganic passivation material, method for forming the same, and inorganic passivation protective film produced therefrom
Abstract
A method for forming an inorganic passivation material is provided. The method includes mixing about 5 to 80 parts by weight of trialkoxysilane, about 10 to 80 parts by weight of tetraalkoxysilane, and about 1 to 30 parts by weight of catalyst to perform a reaction at pH of about 0.05 to 4 to form an inorganic resin material. The inorganic resin material is modified by phosphate ester to form an inorganic passivation material, wherein phosphate ester is about 0.1-10 parts by weight based on 100 parts by weight of the inorganic resin material. An inorganic passivation material and a passivation protective film produced therefrom are also provided.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for forming an inorganic passivation material, comprising: mixing 5 to 80 parts by weight of tetraalkoxysilane, 10 to 80 parts by weight of trialkoxysilane, and 1 to 30 parts by weight of catalyst to perform a reaction at pH of 0.05 to 4, based on a total amount of the tetraalkoxysilane, the trialkoxysilane, and the catalyst, to form an inorganic resin material; and modifying the inorganic resin material by phosphate ester to form an inorganic passivation material, wherein phosphate ester is 0.1 to 10 parts by weight based on 100 parts by weight of the inorganic resin material, wherei
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (21)
Non-Patent Literature (5)
- Chen, "High Molecular-Weight Synthetic Materials Science (I)," Chemical Industrial Press, Jan. 31, 2005, with an English translation, pp. 260-261.
- Chinese Office Action and Search Report dated Nov. 24, 2015, for Chinese Application No. 201210570516.0.
- Chinese Office Action and Search Report for Chinese Application No. 201410045557.7, dated Aug. 26, 2016.
- Díaz et al., "Corrosion resistance of new epoxy-siloxane hybrid coatings. A laboratory study," Progress in Organic Coatings, vol. 69, 2010, pp. 278-286.
- El Aal et al, "Galvanostatic study of the breakdown of Zn passivity by sulphate anions," Corrosion Science, vol. 51, 2009 (Available online May 13, 2009), pp. 1780-1788.