Method for smelting nickel oxide ore and method for charging pellets
Abstract
A method for smelting a nickel oxide ore, wherein the reduction step progresses effectively while maintaining the strength of the pellets, comprises: a pellet production step S 1 for producing pellets from a nickel oxide ore; and a reduction step S 2 for reducing and heating the obtained pellets in a smelting furnace at a predetermined reduction temperature. In the pellet production step S 1, a mixture is formed by mixing materials including said nickel oxide ore without mixing a carbonaceous reducing agent, and the pellets are formed by agglomerating said mixture. In the reduction step S 2, in charging the obtained pellets into the smelting furnace, a carbonaceous reducing agent is spread in advance over the furnace floor of the smelting furnace and the pellets are placed on the carbonaceous reducing agent, and the pellets are reduced and heated in a state where the pellets are covered by the carbonaceous reducing agent.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for charging pellets for smelting by forming pellets from nickel oxide ore, and reducing and heating the pellets with a smelting furnace, the method comprising: a pellet production step of producing pellets from the nickel oxide ore; and a pellet charging step of charging the pellets obtained into a smelting furnace for reducing and heating, wherein the pellet production step forms pellets by making a mixture by mixing raw materials including the nickel oxide ore without mixing in a carbonaceous reducing agent, and then agglomerating the mixture, and wherein the pellet charging step e
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 10,301,704 B2 | Method for smelting saprolite ore | 2019 | 0 |
| US 10,072,313 B2 | Method for smelting nickel oxide ore | 2018 | 0 |
References Cited — Backward Prior Art (13)
Non-Patent Literature (4)
- Extended European Search Report dated Jun. 19, 2017, issued to EP Patent Application No. 15824974.8.
- Gupta, R. C. et al., “The effect of additives and reductants on the strength of reduced iron ore pellet,” ISIJ International 43.12 (2003), pp. 1913-1918. (cited in the Apr. 13, 2017 AU OA).
- International Search Report dated Jul. 28, 2015, issued for PCT/JP2015/068854.
- Office Action dated Apr. 13, 2017, issued to AU Application No. 2015293371.