High zirconia electrically fused cast refractory

1Forward Citations (#51848175 Global)
0.1/yrCitation Velocity (#44438024 Global)
0.84Citation PageRank (#51848175 Global)
13Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A high zirconia electrically fused cast refractory of high electric resistance having long time durability, less suffering from cracking during production and upon temperature rising, excellent in productivity, less forming zircon crystals even upon heating the refractory in itself and when the refractory is in contact with molten glass, generating less cracks even when undergoing heat cycles during operation of a glass melting furnace is provided. A high zirconia electrically fused cast refractory has, as chemical components, 85 to 95% by weight of ZrO 2 , 0.1 to less than 0.8% by weight of Al 2 O 3 , 3.5 to 10.0% by weight of SiO 2 , less than 0.05% by weight of Na 2 O and K 2 O in total, 0.1 to 1.5% by weight of B 2 O 3 , 0.1% by weight or less of MgO, 0.01 to 0.2% by weight of CaO, in the case where any one of BaO and SrO is contained, from 0.05 to 3.0% by weight of BaO or 0.01 to 3.0% by weight of SrO, or in the case where both of them are contained, 0.01% by weight or more of SrO and from 0.01% to 3.0% by weight in total of SrO and BaO, 0.1 to 0.7% by weight of SnO 2 , 0.3% by weight or less of Fe 2 O 3 and TiO 2 in total, less than 0.01% by weight of P 2 O 5 , and less than

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 1.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A high zirconia electrically fused cast refractory with higher electric resistance at high temperature and zircon crystals are less formed even upon heating a refractory in itself or heating under the condition where the refractory is in contact with a molten glass, comprising, as chemical components: 85 to 95% by weight of ZrO 2 0.1 to less than 1.0% by weight of Al 2 O 3 ,

  2. Claim 3Independent Claim

    5 to 10.0% by weight of SiO 2 , less than 0.05% by weight of Na 2 O and K 2 O in total, 0.1 to 1.5% by weight of B 2 O 3 , 0.1% by weight or less of MgO, 0.01 to 0.2% by weight of CaO, in the case where any one of SrO and BaO is contained, 0.05 to 3.0% by weight of BaO or 0.01 to 3.0% by weight of SrO, or in the case where both of them are contained, 0.01% by weight or more of SrO and 0.01 to 3.0% by weight of SrO and BaO in total, 0.01 to 0.7% by weigh

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

Non-Patent Literature (1)

  • International Search Report (ISR) dated Mar. 13, 2015, for PCT/JP2015/056759.