US 9,750,150 B2#107316454 Most CitedActiveUnited States (USPTO)Utility

Break resistant and shock resistant sapphire plate

0Forward Citations (#107316454 Global)
0.0/yrCitation Velocity (#107316454 Global)
0.56Citation PageRank (#107316454 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A break resistant sapphire plate and a corresponding production process. The sapphire plate may include a planar sapphire substrate, and at least one shock absorbing layer arranged on a surface of the substrate. The shock absorbing layer may have a thickness of between 0.1% to 10% of the thickness of the substrate. The production process for producing the sapphire plate may include providing a planar sapphire substrate, and coating at least one surface of the substrate with a shock absorbing layer. The shock absorbing layer may include a layer thickness between 0.1% to 10% of the thickness of the substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A sapphire plate, comprising: a planar sapphire substrate; and at least one shock absorbing layer selectively adhered to portions of a surface of the planar sapphire substrate, wherein the shock absorbing layer has: a layer thickness between 0.1% to 10% of a thickness of the substrate; and at least 50 wt.-% of amorphous aluminum oxide (Al2O3).

  2. Claim 2Depends on #1

    The sapphire plate of claim 1 , wherein the shock absorbing layer thickness is one of: 0.5% to 5%, 0.8% to 3%, 1% to 2%, or 1.2% to 1.5% of the thickness of the substrate.

  3. Claim 3Depends on #1

    The sapphire plate of claim 1 , wherein the thickness of the sapphire substrate is one of: 200 μm to 2 mm, 300 μm to 1.5 mm, 500 μm to 1 mm or 600 μm to 800 μm.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,809,574 AAluminum oxide films for electronic devices197444
US 3,859,714 ABonding of sapphire to sapphire by eutectic mixture of aluminum oxide and zirconium oxide197511
US 5,508,092 AAbrasion wear resistant coated substrate product1996151
JP H098690 APortable communication equipment—70
US 5,942,343 ABonded sapphire, and method of making same199914
DE 69,612,997 T2Verfahren zur herstellung von aluminiumoxidfilmen unter verwendung von dialkylaluminiumalkoxid20019
US 2002052060 A1Method for growing semiconductor layer and method for fabricating semiconductor light emitting elements—2
WO 02,054,718 A2A casing—22
US 2002102819 A1Manufacturing method of compound semiconductor wafer—39
US 6,440,242 B1Method of joining synthetic corundum, method of manufacturing synthetic corundum cell, and synthetic corundum cell20028
US 6,528,123 B1Coating system to permit direct brazing of ceramics200356
US 2003045103 A1Nitride III-V compound semiconductor substrate, its manufacturing method, manufacturing method of a semiconductor light emitting device, and manufacturing method of a semiconductor device—29
US 6,627,319 B2Glazing with a functional, especially hydrophobic, mesoporous coating200326
US 2003228476 A1Methods of changing the visible light transmittance of coated articles and coated articles made thereby—73
US 2004102229 A1Casing—20
US 6,916,542 B2Coated articles having a protective coating and cathode targets for making the coated articles200556
US 6,962,759 B2Method of making coated articles having an oxygen barrier coating and coated articles made thereby200540
DE 112004001032 T5Verfahren zum Verbinden von Keramik: Reaktions-Diffusionsbinden—16
US 7,125,926 B2Surface treatment agent comprising inorganic-organic hybrid material200630
US 2007048526 A1Recycling compatible hard coating—10
US 2007085163 A1Gallium nitride thin film on sapphire substrate having reduced bending deformation—8
US 2007224357 A1Coating stack comprising a layer of barrier coating—9
US 7,311,961 B2Method of making coated articles and coated articles made thereby200743
JP 2008111984 APortable electronic device—38
US 2008139885 A1Autoclavable antireflective coatings for endoscopy windows and related methods—9
WO 2009/025842 A1Laminated display window and device incorporating same—12
US 2009090241 A1Gas separation membranes containing a microporous silica layer based on silica doped with a trivalent element—18
US 7,584,689 B2Transparent ceramic composite armor200931
US 2009263651 A1Optically transparent resilient laminate materials and methods of manufacture—17
US 2010027383 A1Transparent member, timepiece, and method of manufacturing a transparent member—34

Non-Patent Literature (5)

  • Barbour JD et al., "The mechanical properties of alumina films formed by plasma deposition and by ion irradiation of sapphire," Nuclear Instruments & Methods in Physics Research, Section-B:Beam Interactions with Materials and Atoms, Elsevier, Amsterdam, NL, vol. 166-167, May 1, 2000, pp. 140-147.
  • Barbour JD et al., “The mechanical properties of alumina films formed by plasma deposition and by ion irradiation of sapphire,” Nuclear Instruments & Methods in Physics Research, Section—B:Beam Interactions with Materials and Atoms, Elsevier, Amsterdam, NL, vol. 166-167, May 1, 2000, pp. 140-147.
  • Chaudhari, P. et al., Heteroepitaxial Silicon Film Growth at 600C. From an Al-Si Eutectic Melt, pp. 5368-5371, Mar. 19, 2010, Thin Solid Films 518, Elsevier, US.
  • Chaudhari, P. et al., Heteroepitaxial Silicon Film Growth at 600C. From an Al—Si Eutectic Melt, pp. 5368-5371, Mar. 19, 2010, Thin Solid Films 518, Elsevier, US.
  • Feng et al., "Strengthening sapphire at elevated temperatures b Si02 films," Applied Surface Science, Elsevier, Amsterdam, NL, vol. 253, No. 12, Mar. 13, 2007, pp. 5365-5367.