Thin-film packaging method and organic light-emitting device

3Forward Citations (#33638190 Global)
0.3/yrCitation Velocity (#23658686 Global)
1.02Citation PageRank (#40691121 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A thin-film packaging method and an organic light-emitting device are provided. The method includes following steps: forming an OLED layer on a TFT substrate, forming a first inorganic packaging layer on the OLED layer, forming a coupling agent unit on the first inorganic packaging layer, and forming an organic packaging layer on the coupling agent unit. Wherein, the organic packaging layer includes a buffer sublayer and a resist sublayer sequentially formed. The coupling agent unit generates chemical reactions with the first inorganic packaging layer and the buffer sublayer in order to increase an adhesive strength between the first inorganic packaging layer and the organic packaging layer so that they are not easily to be separated, and have a good water and oxygen insulation property.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A thin-film packaging method, comprising following steps: forming an Organic Light-Emitting-Diode (OLED) layer on a Thin-Film-Transistor (TFT) substrate; forming a first inorganic packaging layer on the OLED layer; forming a coupling agent unit on the first inorganic packaging layer; and forming an organic packaging layer on the coupling agent unit; wherein, the organic packaging layer includes a buffer sublayer and a resist sublayer sequentially formed on the coupling agent unit, the coupling agent unit generates chemical reacts with the first inorganic packaging layer and the buffer sublayer