An oxide semiconductor crystallization method may include depositing an In—Ga—Zn oxide over the substrate while heating a substrate to a temperature of 200 to 300° C., and heat-treating the deposited In—Ga—Zn oxide at a temperature of 200 to 350° C., thereby forming an oxide semiconductor layer crystallized throughout an entire thickness thereof.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 6.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for crystallizing an oxide semiconductor layer, the method comprising: depositing an In—Ga—Zn oxide over a substrate using an In—Ga—Zn target while heating the substrate to a first low temperature of 200 to 300° C., wherein an atomic % ratio of In, Ga, Zn of the In—Ga—Zn target is 1:1:1.10˜1.25; and heat-treating the deposited In—Ga—Zn oxide at a second low temperature of 200 to 350° C. to form a crystallized oxide semiconductor throughout an entire thickness of the deposited In—Ga—Zn oxide.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the depositing the In—Ga—Zn oxide is carried out for 2 to 5 minutes.

  3. Claim 3Depends on #1

    The method according to claim 1 , wherein the depositing the In—Ga—Zn oxide is carried out using a DC sputtering.