Patents
US 9,732,172 B2#44564449 Most CitedActiveUnited States (USPTO)Utility

Ethylene/1-hexene or ethylene/1-butene copolymer having excellent processibility and environmetal stress crack resistance

2Forward Citations (#44564449 Global)
0.2/yrCitation Velocity (#31865961 Global)
0.90Citation PageRank (#47636010 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to an ethylene/1-hexene or ethylene/1-butene copolymer having excellent processibility. The ethylene/1-hexene or ethylene/1-butene copolymer according to the present invention has high molecular weight and wide molecular weight distribution, and thus excellent processibility, and has excellent environmental stress crack resistance, and thus, may be applied for a high inner pressure heating pipe, a mining pipe, or a large-diameter pipe, and the like.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An ethylene/1-butene copolymer having: weight average molecular weight(g/mol) of 10,000 to 400,000, molecular weight distribution (Mw/Mn, PDI) of 2 to 30, density (g/cm 3 ) of 0.930 to 0.950, MFR 5 (g/10 min, measured at 190° C. by ASTM 1238) of 0.1 to 5, melt flow rate ratio (MFR 21.6 /MFR 5 , measured at 190° C. by ASTM 1238) of 10 to 200, and an environmental stress crack resistance (ESCR) of 400 hours to 20,000 hours, as measure by full notch creep test (FNCT) according to ISO 16770 at 4.0 MPa and 80° C.

  2. Claim 2Depends on #1

    The copolymer according to claim 1 , wherein the environmental stress crack resistance (ESCR) measured by full notch creep test (FNCT) according to ISO 16770 at 4.0 MPa and 80° C. is 600 hours to 8,760 hours.

  3. Claim 3Depends on #1

    The copolymer according to claim 1 , wherein the weight average molecul

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,935,474 AProcess and catalyst for producing polyethylene having a broad molecular weight distribution1990244
US 5,914,289 ASupported metallocene-alumoxane catalysts for the preparation of polyethylene having a broad monomodal molecular weight distribution1999106
KR 20000069979 AMetallocenes and catalysts for olefin-polymerisation—8
US 6,185,349 B1Multimodal polymer composition200171
JP 2002504958 A異なる触媒活性部位を有する触媒を用いる多段階重合プロセス—5
EP 1,231,238 A1Multimodal polyethylene resin composition for fibre supporting elements for fibre optic cables—4
US 6,441,096 B1Polymer composition for pipes200249
KR 20040037067 AInjection blow moulded single layer metallocene polyethylene container—3
US 6,756,455 B2High-temperature solution process for polyolefin manufacture200420
KR 20040076965 AA supported multinuclear metallocene catalysts for olefin polymerization and a process for preparing the same—74
US 2004181010 A1Polyethylene pipe resins and production thereof—15
US 6,828,394 B2Mixed metallocene catalyst systems containing a poor comonomer incorporator and a good comonomer incorporator200492
US 6,841,631 B2Catalyst composition, method of polymerization, and polymer therefrom200593
KR 20050024287 AHigh-temperature olefin polymerisation process in solution—21
US 6,894,128 B2Catalyst composition, method of polymerization, and polymer therefrom200593
US 2005228139 A1Polyethylene pipe having better melt processibility and high resistance to stress and method of preparing the same using metallocene catalyst—20
US 2006079656 A1Olefin polymers, method of making, and use thereof—11
US 7,037,977 B2Polyethylene pipe resins and production thereof200619
KR 20060087890 AMixed supported metallocene catalysts, method for preparing the same, polyolefins and method for manufacturing the polyolefins using the same—16
US 2006183631 A1Supported metallocene catalyst and method of preparing ethylene-based copolymer using the same—36
KR 100,646,249 B1Polyethylene Pipe Having Good Melt Processibilty and High Resistance to Stress and Method for Preparing the Same Using Metallocene Catalysts20066
CN 1,906,220 APolyethylene pipe having better melt processibility and high resistance to stress and method of preparing the same using metallocene catalyst—12
JP 3,968,449 B2ポリエチレンパイプ樹脂およびそれらの製造20071
JP 2007218324 APolyethylene pipe—11
US 2007273066 A1Lldpe Pressure Pipe—12
KR 20070117565 AOlefin polymerization catalyst on plasma-contacted support—1
US 2008196922 A1Outer Sheath Layer for Power or Communication Cable—21
KR 20080097949 APolyolefin and preparation method thereof—23

Non-Patent Literature (2)

  • Helmut G. Alt et al.: "Polymerization of ethylene with metallocene/methylaluminoxane catalysts supported on polysiloxane micro gels and silica", Journal of Organometallic Chemistry 568 (1998) pp. 263-269.
  • Walter Kaminsky: "Highly active metallocene catalysts for olefin polymerization", J. Chem. Soc., Dalton Trans., 1998, pp. 1413-1418.