Patents
US 9,725,791 B2#47297836 Most CitedActiveUnited States (USPTO)Utility

Zirconium alloys with improved corrosion/creep resistance due to final heat treatments

1Forward Citations (#47297836 Global)
0.1/yrCitation Velocity (#44141196 Global)
0.98Citation PageRank (#42831226 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Articles, such as tubing or strips, which have excellent corrosion resistance to water or steam at elevated temperatures, are produced from alloys having 0.2 to 1.5 weight percent niobium, 0.01 to 0.6 weight percent iron, and optionally additional alloy elements selected from the group consisting of tin, chromium, copper, vanadium, and nickel with the balance at least 97 weight percent zirconium, including impurities, where a necessary final heat treatment includes one of i) a SRA or PRXA (15-20% RXA) final heat treatment, or ii) a PRXA (80-95% RXA) or RXA final heat treatment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A zirconium-based alloy having one of improved corrosion resistance and improved creep resistance, for use in an elevated temperature environment of a nuclear reactor, comprising an alloying composition: 0.2 to 1.5 weight percent niobium; 0.01 to 0.6 weight percent iron; 0.0 to 0.8 weight percent tin; 0.0 to 0.5 weight percent chromium; 0.0 to 0.3 weight percent copper; 0.0 to 0.3 weight percent vanadium; 0.0 to 0.1 weight percent nickel; and a balance at least 97 weight percent zirconium, including impurities, the zirconium-based alloy formed by a process, comprising: (a) melting the alloying

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,085,059 AFuel element for nuclear reactors196329
US 4,212,686 AZirconium alloys198046
US 4,562,713 ACold pilger mill198625
US 4,649,023 AProcess for fabricating a zirconium-niobium alloy and articles resulting therefrom198794
JP S63213629 AZirconium based alloy—9
US 4,775,508 AZirconium alloy fuel cladding resistant to PCI crack propagation198834
US 4,814,136 AProcess for the control of liner impurities and light water reactor cladding198911
JP H01119650 AManufacture of channel box for nuclear reactor fuel assembly—14
US 4,938,920 ANuclear reactor fuel assembly199036
US 4,963,323 AHighly corrosion-resistant zirconium alloy for use as nuclear reactor fuel cladding material199021
US 4,992,240 AAlloys based on zirconium having proportional amount of tin, iron, chromium and oxygen199141
EP 0,425,465 A1A method of manufacturing cladding tubes for fuel rods for nuclear reactors—16
US 5,017,336 AZironium alloy for use in pressurized nuclear reactor fuel components199121
US 5,023,048 ARod for a fuel assembly of a nuclear reactor resisting corrosion and wear199127
US 5,112,573 AZirlo material for light water reactor applications199230
US 5,125,985 AProcessing zirconium alloy used in light water reactors for specified creep rate199248
US 5,211,774 AZirconium alloy with superior ductility199331
US 5,230,758 AMethod of producing zirlo material for light water reactor applications199330
US 5,254,308 AZirconium alloy with improved post-irradiation properties199344
US 5,266,131 AZirlo alloy for reactor component used in high temperature aqueous environment199319
US 5,341,407 AInner liners for fuel cladding having zirconium barriers layers199427
US 5,366,690 AZirconium alloy with tin, nitrogen, and niobium additions199428
US 5,373,541 ANuclear fuel rod and method of manufacturing the cladding of such a rod199420
US 5,519,748 AZircaloy tubing having high resistance to crack propagation199628
US 5,560,790 AZirconium-based material, products made from said material for use in the nuclear reactor core, and process for producing such products199652
US 5,618,356 AMethod of fabricating zircaloy tubing having high resistance to crack propagation199718
US 5,620,536 AManufacture of zirconium cladding tube with internal liner199728
US 5,648,995 AMethod of manufacturing a tube for a nuclear fuel assembly, and tubes obtained thereby199719
US 5,681,404 AMethod of fabricating Zircaloy tubing having high resistance to crack propagation199715

Non-Patent Literature (5)

  • Davis et al., "ASM International Handbook," vol. 2, Oct. 1990, pp. 661-669.
  • European Patent Office, Extended European Search Report for European Application No. 16000804.1, mailed Jul. 7, 2016.
  • International Preliminary Report on Patentability for PCT/US2012/038471 dated Dec. 17, 2013 (Form PCT/IB/373, PCT/ISA/237).
  • Jung et al., "Behavior of a recrystallization in HANA-4 and HANA-6 zirconium-based alloys", Journal of Alloys and Compounds 479 (2009), pp. 423-426.
  • Jung et al., "Effect of Cr on the creep properties of zirconium alloys", Journal of Nuclear Materials 396 (2010), pp. 303-306.