Negative active material for secondary battery and secondary battery using the same
Abstract
The present invention provides a negative active material for a secondary battery with an improved expansion rate, which is formed by a formula below, and in which an expansion rate of the negative active material after 50 cycles is 70 to 150%, and an amorphization degree on a matrix within an alloy has a range of 25% or more, and Si has a range of 60 to 70%, Ti has a range of 9 to 14%, Fe has a range of 9 to 14%, and Al has a range larger than 1% and less than 20%. Formula: Si x Ti y Fe z Al u (x, y, z, and u are at %, x: 1−(y+z+u)).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 5.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A negative active material for a secondary battery, which is an alloy formed by a chemical formula below, and in which an amorphization degree of a fine crystalline region on a matrix within the alloy is 25% or more: Si x Ti y Fe z Al u , where x, y, z, and u are at %, x: 1−(y+z+u), y: 0.09 to 0.14, z: 0.09 to 0.14, and u: larger than 0.01 and less than 0.2, wherein an expansion rate of the negative active material after 50 cycles has a range of 70 to 150% and wherein a ratio of Ti to Fe in the negative active material for the secondary battery has a range of 2:1 to 1:2.
- Claim 2Depends on #1
The negative active material of claim 1 , wherein Al in the negative active material for the secondary battery has a range of 5 to 19% based on atom (%) (at (%)).
- Claim 3Depends on #2
The negative active material of claim 2 , wherein Al in the negative
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗