Patents
US 9,718,249 B2#12213772 Most CitedActiveUnited States (USPTO)Utility

Laminated aluminum oxide cover component

9Forward Citations (#12213772 Global)
1.0/yrCitation Velocity (#6796852 Global)
1.54Citation PageRank (#22075734 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A cover glass for an electronic display comprises a plurality of layers of sapphire material, each of the layers having a substantially single crystal plane orientation, with adjacent layers having different substantially single crystal plane orientations. One or more interface layers are defined between adjacent layers of the sapphire material, with the adjacent layers of sapphire material bonded together at the one or more interface layers. A display window is defined in the cover glass, and configured for viewing a viewable area of the electronic display through the plurality of layers of the sapphire material bonded together at the one or more interface layers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 9.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A cover glass for an electronic display, the cover glass comprising: a plurality of sapphire sheets directly bonded together by hydrogen bonds at a planar interface between adjacent sapphire sheets; and a display window defined in the cover glass, the display window configured for viewing the electronic display through the plurality of sheets of substantially single crystal sapphire; wherein each of the sapphire sheets has a substantially single crystal plane orientation; and adjacent sapphire sheets have different crystal plane orientations.

  2. Claim 2Depends on #1

    The cover glass of claim 1 , wherein the adjacent sapphire sheets have substantially orthogonal crystal plane orientations.

  3. Claim 3Depends on #2

    The cover glass of claim 2 , wherein the adjacent sapphire sheets comprise alternating A plane and C plane orientations.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,713,877 AMethod of strengthening ceramic bodies and strengthened ceramic bodies produced thereby197319
US 3,736,171 AMethod of strengthening ceramics using ion exchange19736
US 3,809,574 AAluminum oxide films for electronic devices197444
US 3,859,714 ABonding of sapphire to sapphire by eutectic mixture of aluminum oxide and zirconium oxide197511
US 4,043,638 ALiquid crystal display mounted behind a front glass197725
US 4,339,300 AProcess for smoothing surfaces of crystalline materials198238
US 4,675,089 ALow temperature deposition method for high quality aluminum oxide films198736
JP H0266159 AFormation of aluminum nitride layer—5
US 5,508,092 AAbrasion wear resistant coated substrate product1996151
JP H098690 APortable communication equipment—70
WO 9,720,963 A1Process for the preparation of aluminum oxide film using dialkylaluminum alkoxide—9
US 5,935,723 AEnvironmentally resistant, infrared-transparent window structure199920
US 5,942,343 ABonded sapphire, and method of making same199914
US 6,012,303 AEutectic bonding of single crystal components200020
DE 69,612,997 T2Verfahren zur herstellung von aluminiumoxidfilmen unter verwendung von dialkylaluminiumalkoxid20019
WO 02,054,718 A2A casing—22
US 6,440,242 B1Method of joining synthetic corundum, method of manufacturing synthetic corundum cell, and synthetic corundum cell20028
US 6,475,820 B2Method for growing semiconductor layer and method for fabricating semiconductor light emitting elements20026
US 6,528,123 B1Coating system to permit direct brazing of ceramics200356
US 2003044577 A1Method and apparatus for multilayer optical articles—21
US 6,627,319 B2Glazing with a functional, especially hydrophobic, mesoporous coating200326

Non-Patent Literature (5)

  • Barbour JD et al., “The mechanical properties of alumina films formed by plasma deposition and by ion irradiation of sapphire,” Nuclear Instruments & Methods in Physics Research, Section—B:Beam Interactions with Materials and Atoms, Elsevier, Amsterdam, NL, vol. 166-167, May 1, 2000, pp. 140-147.
  • Chaudhari, P. et al., Heteroepitaxial Silicon Film Growth at 600C From an Al—Si Eutectic Melt, pp. 5368-5371, Mar. 19, 2010, Thin Solid Films 518, Elsevier, US.
  • Feng et al., “Strengthening sapphire at elevated temperatures b Si02 films,” Applied Surface Science, Elsevier, Amsterdam, NL, vol. 253, No. 12, Mar. 13, 2007, pp. 5365-5367.
  • International Search Report and Written Opinion, PCT Application No. PCT/EP2014/054819, 12 pages, Apr. 30, 2014.
  • International Search Report and Written Opinion, PCT Application No. PCT/EP2014/054820, 11 pages, Apr. 30, 2014.