Abstract
The present invention is a composition comprising a stable aqueous dispersion of polymer particles and a sorbate ester, which is a liquid at 20° C. and has a molecular weight in the range of 125 to 500 g/mol. The composition of the present invention provides a way to enhance film formation of coatings prepared using relatively high T g latexes without the aid of high volatile organic content (VOC) coalescents.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 2.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A composition comprising a stable aqueous dispersion of polymer particles, from 0.5 to 35 weight percent of a sorbate ester or sorbamide coalescent, based on the weight of the polymer particles, and from 10 ppm to 1 weight percent of a radical mediator, based on the weight of the composition, wherein the coalescent is imbibed in the polymer particles, wherein at least 60% of the coalescent is incorporated into the polymer particles; and wherein radical mediator is a hindered amine, a hindered N-oxide, a thiol, an amino polycarboxylic acid or a salt thereof, a polyphosphate, or a phenol, or a c
- Claim 2Depends on #1
The composition of claim 1 wherein the coalescent is characterized by the following formula: where R
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (6)
Non-Patent Literature (1)
- English machine translation of Sato et al. (JP 2001-181348); translated Jul. 6, 2016.