Patents
US 9,714,192 B2#18787111 Most CitedActiveUnited States (USPTO)Utility

Ion exchangeable glass with advantaged stress profile

6Forward Citations (#18787111 Global)
0.7/yrCitation Velocity (#11671395 Global)
1.28Citation PageRank (#29348121 Global)
28Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Ion exchangeable glass compositions that develop concentration profiles and stress profiles that have higher magnitudes of concentration and compressive stress profiles than those provided by the error function (erfc)-shaped compressive stress profile for similar surface concentrations of stress-inducing components such as K + or K 2 O and stresses. The advantaged stress profile is the result of a glass composition that is low in K 2 O (or potassium) in the base glass prior to ion exchange. A glass comprising lower amounts of K + or K 2 O has a stronger dependence of diffusivity on concentration, leading to a non-erfc-shaped concentration profile. Several glass compositions that contain low amounts of K + or K 2 O exhibit this beneficial effect, whereas other glasses containing higher amounts of K + or K 2 O do not exhibit this effect.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 6.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An alkali aluminosilicate glass comprising: at least about 50 mol % SiO 2 , from about 9 mol % to about 22 mol % Al 2 O 3 ; from about 3 mol % to about 10 mol % B 2 O 3 ; from greater than 14 mol % to about 20 mol % Na 2 O; from 0 mol % to 1 mol % K 2 O; MgO, and ZnO, wherein MgO+ZnO≧0.1 mol %, 0 mol %≦MgO≦6 mol %, and 0 mol %≦ZnO≦6 mol %, and having a layer under a compressive stress CS(d) that varies as a function of depth d from a surface of the glass to a depth of layer DOL, wherein 1.2·CS erfc (d)≧CS(d)≧1.1·CS erfc (d) at 0.4·DOL≦d≦0.6·DOL, where CS erfc (d) is a compressive stress at dep

  2. Claim 2Depends on #1

    The alkali aluminosilicate glass of claim 1 , wherein the glass comprises alkali metal oxides, and wherein K 2 O is present in a molar concentration that is less than about 7% of the total

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (28)

PatentTitleYearCitations
US 2003220183 A1Glass composition, glass article, glass substrate for magnetic recording media, and method for producing the same—69
US 2005003136 A1Glass composition including zirconium, chemically strengthened glass article, glass substrate for magnetic recording media, and method of producing glass sheet—53
US 2005250639 A1Lithium-aluminosilicate flat float glass—138
US 2008286548 A1Down-drawable, chemically strengthened glass for cover plate—161
US 2009197088 A1Tempered glass substrate and method of producing the same—170
US 2009220761 A1Ion exchanged, fast cooled glasses—189
US 2010035745 A1Tempered glass substrate—148
US 2010291353 A1Method of separating strengthened glass—101
US 2011014475 A1Reinforced glass, reinforced glass substrate, and method for producing the same—117
US 2011281093 A1Damage-resistant glass articles and method—84
US 2011294648 A1Ion exchangeable glasses—121
US 8,187,987 B2Durable glass housings/enclosures for electronic devices201247
US 2012171497 A1Cover glass and method for producing same—59
US 2012194974 A1Enhanced chemical strengthening glass for portable electronic devices—85
US 2012196110 A1Tempered glass and tempered glass sheet—71
KR 20120128657 AEnhanced chemical strengthening glass of covers for portable electronic devices—5
US 2013004758 A1Ion exchangeable glass with high compressive stress—106
US 8,349,455 B2Glass and chemically tempered glass201320
US 2013224492 A1Ion exchanged glasses via non-error function compressive stress profiles—147
US 2013236666 A1Glass with surface and central regions under compression—28
US 2014120279 A1Glass packaging ensuring container integrity—23
US 2014141226 A1Ion exchangeable glasses having high hardness and high modulus—18
US 2014186632 A1Zircon compatible, ion exchangeable glass with high damage resistance—10
US 8,889,575 B2Ion exchangeable alkali aluminosilicate glass articles201410

Non-Patent Literature (3)

  • Helfferich et al.; "Ion Exchange Kinetics. A Nonlinear Diffusion Problem"; The Journal of Chemical Physics, vol. 28, No. 3, Mar. 1958; pp. 418-424.
  • René Gy; "Ion exchange for glass strengthening"; Materials Science and Engineering B 149 (2008); pp. 159-165.
  • Roger Araujo; "Interdiffusion in a one-dimensional interacting system"; Journal of Non-Crystalline Solids 152 (1993); pp. 70-74.