Abstract

A method for the low-pressure carbonitriding of steel parts, in particular parts used in the manufacture of automobiles, comprises a heating step that includes a simple heating phase (M) followed by an initial nitridation phase (Ni) from a temperature between 700° C. to 750° C. to a temperature between 860° and 1000° C. and carried out using a reduced temperature gradient relative to the simple heating phase. Additionally, alternate cementing (C1-Cn) and nitridation (N1-Nn) steps are performed at constant temperature, wherein the final nitridation step is accompanied with a decrease in temperature immediately before quenching (T).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A low-pressure carbonitriding method of steel parts comprising alternate cementation and nitriding steps at constant temperature, preceded by a heating step comprising a simple heating phase followed by an initial nitriding phase during which the heating is carried on, and followed by a quenching step, wherein during the initial nitriding phase, the heating is performed with a decreased temperature gradient as compared with the simple heating phase.

  2. Claim 2Depends on #1

    The low-pressure carbonitriding method of claim 1 , wherein the initial nitriding phase comprises a temperature stage.

  3. Claim 3Depends on #1

    The low-pressure carbonitriding method of claim 1 , wherein the initial nitriding phase is carried out with a temperature gradient in the range from 3.5° C./min to 16° C./min.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (4)

  • Search report issued in PCT/EP2012/069888 on Jan. 10, 2013.
  • Search report issued in PCT/EP2012/069889 on Jan. 14, 2013.
  • Search Report issued in PCT/EP2012/069890 on Jan. 15, 2013.
  • von Stark, A. et al., Handbook of Thermoprocessing Technologies: Fundamentals, Processes, Components, Safety, Vulkan-Verlag GmbH, 2005, p. 509.