Patents
US 9,708,216 B2#21102016 Most CitedActiveUnited States (USPTO)Utility

Phosphorous containing glass having antimicrobial efficacy

5Forward Citations (#21102016 Global)
0.6/yrCitation Velocity (#14365684 Global)
1.44Citation PageRank (#24250240 Global)
18Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A strengthened antimicrobial glass including greater from about 50.0 mol. % to about 65.0 mol. % SiO 2 , about 14.0 mol. % to about 22.0 mol. % Al 2 O 3 , about 14.0 mol. % to about 22.0 mol. % R 2 O, wherein R is an alkali metal, and about 4.0 mol. % to 10.0 mol. % P 2 O 5 . The glass may have a compressive stress layer having a thickness of greater than or equal to about 20 μm to less than or equal to about 60 μm and having a compressive stress of greater than or equal to about 700 MPa. The glass may have an antimicrobial activity greater than or equal to about 1.0 log kill at about 23° C. and about 40.0% relative humidity. A method for making the glass may include obtaining a glass article, strengthening the glass article by contact with a first ion-exchange liquid, and contacting the glass article with second ion-exchange liquid comprising an antimicrobial agent.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 5.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A strengthened antimicrobial glass comprising: greater than or equal to about 50.0 mol. % to less than or equal to about 65.0 mol. % SiO 2 ; greater than or equal to about 14.0 mol. % to less than or equal to about 22.0 mol. % Al 2 O 3 ; greater than or equal to about 14.0 mol. % to less than or equal to about 22.0 mol. % R 2 O, wherein R is an alkali metal; and greater than or equal to about 4.0 mol. % to less than or equal to about 10.0 mol. % P 2 O 5 , wherein: the glass comprises a compressive stress layer having a thickness of greater than or equal to about 20 μm and having a surface comp

  2. Claim 2Depends on #1

    The glass of claim 1 , wherein

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (18)

PatentTitleYearCitations
US 3,357,876 AMethod of strengthening a glass article by ion exchange1967176
US 4,055,703 AIon exchange strengthened glass containing P2 O51977110
JP H01167245 AGlass composition for chemical reinforcement—21
WO 2006/058906 A1Process for the production of silver-container prosthetic devices—26
US 7,232,777 B1Yarns and fabrics having a wash-durable antimicrobial silver particulate finish200723
US 2009197048 A1Damage resistant glass article for use as a cover plate in electronic devices—201
US 2011294648 A1Ion exchangeable glasses—121
US 2012034435 A1Coated, antimicrobial, chemically strengthened glass and method of making—120
US 2013122284 A1Ion exchangeable glass with high crack initiation threshold—77
US 2013122313 A1Ion exchangeable glass with high crack initiation threshold—30
US 2014356605 A1Antimicrobial Articles and Methods of Making and Using Same—31
US 2014370302 A1Antimicrobial Glass Articles with Improved Strength and Methods of Making and Using Same—26
US 2014370303 A1Antimicrobial glass articles and methods of making and using same—25
US 8,973,401 B2Coated, antimicrobial, chemically strengthened glass and method of making20158
US 2015225288 A1Glass with enhanced strength and antimicrobial properties, and method of making same—13
US 2015225287 A1Antimicrobial glass articles and methods of making and using same—12
US 2015239777 A1High strength antimicrobial glass—18
US 9,156,724 B2Ion exchangeable glass with high crack initiation threshold201551

Non-Patent Literature (3)

  • LV et al; "Antibiotic Glass Slide Coated With Silver Nanoparticles and Its Antimicrobial Capabilities"; Polym. Adv. Technol. 2008; 19: 1455-1460.
  • Nunzio, Brovarone, Spriano, Milanese, Verne, Bergo, Maina, Spinelli, "Silver containing bioactive glasses prepared by molten salt ion-exchange", Journal of the European Ceramic Society, 24 (2004) 2935-2942.
  • Verne et al; "Surface Silver-Doping of Biocompatible Glass to Induce Antibacterial Properties. Part I: Massive Glass"; J. Mater. Sci.: Mater. Med. (2009) 20: 733-740.