Method for producing inorganic fiber-bonded ceramic material

0Forward Citations (#62183068 Global)
0.0/yrCitation Velocity (#62183068 Global)
0.56Citation PageRank (#62183068 Global)
12Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Provided is a method for producing an inorganic fiber-bonded ceramic material, which can produce, at a high yield, an inorganic fiber-bonded ceramic material with fewer defects, and with an end part and a central part equivalent to each other in microstructure and mechanical properties, and also makes it possible to increase the ceramic material in size. The method for producing an inorganic fiber-bonded ceramic material is characterized in that it includes: a first pressing step of setting, in a carbon die, a laminate to be surrounded by a ceramic powder, the laminate obtained by stacking a coated inorganic fiber shaped product including an inorganic fiber part of inorganic fibers that have a pyrolysis initiation temperature of 1900° C. or lower, and a surface layer of an inorganic substance for bonding the inorganic fibers to each other, and pressing the laminate at a temperature of 1000 to 1800° C. and a pressure of 5 to 50 MPa in an inert gas atmosphere; and a second pressing step of pressing a ceramic coated laminate obtained in the first pressing step at a temperature of 1600 to 1900° C., which is higher than that in the first pressing step, and at a pressure of 5 to 100 MPa

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing an inorganic fiber-bonded ceramic part, comprising: a first pressing step of setting a laminate in a carbon die so as to be surrounded by an alumina powder, the laminate being obtained by stacking a coated inorganic fiber shaped product including an inorganic fiber part formed of inorganic fibers having a pyrolysis initiation temperature of 1900° C. or lower and a surface layer formed of an inorganic substance for bonding the inorganic fibers to each other, and pressing the laminate at a temperature of 1000 to 1800° C. and a pressure of 5 to 50 MPa in an inert gas atmosp

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (3)

  • "Hot pressing", Wikipedia, Aug. 9, 2016, pp. 1-4, XP055314308.
  • ANONYMOUS: "Hot pressing - Wikipedia", 9 August 2016 (2016-08-09), XP055314308, Retrieved from the Internet <URL:https://en.wikipedia.org/wiki/Hot_pressing> [retrieved on 20161026]
  • Ishikawa et al. “JP 07-069747, machine translation”, Published Apr. 14, 1995.