Patents
US 9,701,072 B2#12219641 Most CitedActiveUnited States (USPTO)Utility

Methods of repairing matrix cracks in melt infiltrated ceramic matrix composites

9Forward Citations (#12219641 Global)
1.0/yrCitation Velocity (#6804634 Global)
1.52Citation PageRank (#22301695 Global)
21Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of repairing matrix microcracks in MI-CMC components includes heating “free” silicon phase present within the cracked matrix portion of the component to a temperature above the melting point of the silicon phase. During heating of the component an additional source of silicon phase is supplied to the component. The atmosphere about the component is controlled during the heating of the component. The MI-CMC component is cooled below the melting point of the silicon phase to cool and solidify the silicon phase that has migrated into the microcracks to thereby bond the crack faces together.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of repairing one or more cracks in a matrix portion of a melt-infiltrated ceramic matrix composite (CMC) component with a matrix portion comprising substantially silicon carbide and areas of silicon phase dispersed within the silicon carbide, the method comprising: heating the melt-infiltrated CMC component to a first temperature above the melting point of the silicon phase to form molten silicon phase within the matrix portion, wherein the molten silicon phase flows into the one or more cracks; controlling the atmosphere about the melt-infiltrated CMC component while heating the melt

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
US 4,737,328 AInfiltration of material with silicon198849
CN 1,220,649 AOpen-cell expanded ceramic with high level of strength,and process for production thereof—13
US 5,962,103 ASilicon carbide-silicon composite having improved oxidation resistance and method of making199977
US 5,965,266 AComposite material protected against oxidation by a self-healing matrix, and a method of manufacturing it1999108
US 6,024,898 AArticle and method for making complex shaped preform and silicon carbide composite by melt infiltration2000147
US 6,063,514 AGas-tight article and a producing process thereof200015
CN 1,318,041 AMethod for curing cracks in ceramic shaped bodies and shaped bodies treated in such manner—3
US 6,403,158 B1Porous body infiltrating method200280
US 2003004050 A1Fiber-reinforced material composed, at least in a surface region, of a metal/ceramic composite, molding composed of the fiber-reinforced material and method of producing the fiber-reinforced material—10
US 6,635,339 B1Open-cell expanded ceramic with a high level of strength, and process for the production thereof200348
US 6,638,568 B1Method for curing cracks in ceramic shaped bodies and shaped bodies treated in such a manner20033
US 2006163773 A1Method for performing silicon melt infiltration of ceramic matrix composites—37
US 2007099527 A1Method and reactor to coat fiber tows and article—52
US 2010009143 A1Process for manufacturing a part made of a ceramic matrix composite containing matrix phases for healing and deflecting cracks—19
US 7,658,781 B1Silicon-containing composite bodies, and methods for making same201023
US 2010059166 A1Methods of repairing a substrate—5
US 2010279845 A1Process of producing ceramic matrix composites—30
US 2013022471 A1Methods for repairing a turbine airfoil constructed from cmc material—18
US 2013096217 A1Method for fabricating a ceramic material—12
WO 2013/079853 A1Cmc material part manufacture method—6
US 8,728,261 B2Method for producing ceramic joined body20141

Non-Patent Literature (5)

  • Kelina, et al; "Resistance of Si3N4/Cf Ceramic-Matrix Composites to High-Temperature Oxidation," Refractories and Industrial Ceramics, vol. 44, Issue 4 (Jul.-Aug 2003), pp. 249-253.
  • Nakao, et al; "SiC nanometer sizing effect on self healing ability of structural ceramics," Ceramic Engineering and Science Proceedings, vol. 30, Issue 2, 2010, pp. 137-142.
  • PCT search report and written opinion issued in relation to corresponding application PCT/US14/57571 on Jan. 5, 2015.
  • Quemard, et al; "High potential of composites with carbon fibers and a self-sealing ceramic matrix in moist environments under high pressures at 600 degrees C," Ceramic Transactions, vol. 215, 2010, pp. 125-134.
  • Smeacetto, et al; "Protective Coatings for Carbon Bonded Carbon Fibre Composites," Ceramics International, vol. 34, Issue 5, Jul. 2008, pp. 1297-1301.