Glass composition, glass composition for chemical strengthening, strengthened glass article, and cover glass for display
Abstract
Provided is a glass composition containing, in mass %: 58 to 64% SiO 2 ; 8 to 12% Al 2 O 3 ; 6 to 10% MgO; 0 to 1% CaO; 18 to 24% Na 2 O; 0 to 3% K 2 O; 0 to 2% TiO 2 ; and 0 to 3% ZrO 2 . The total content of MgO, CaO, SrO, and BaO is in a range of 7 to 12%. This glass composition is suitable for production by a float process and for chemical strengthening.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 1.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A glass composition comprising, in mass %: 58 to 64% SiO 2 ; 8 to 12% Al 2 O 3 ; 6 to 10% MgO; 0 to 1% CaO; 18 to 24% Na 2 O; 0 to 3% K 2 O; 0 to 2% TiO 2 ; and 0 to 3% ZrO 2 , wherein a total content of MgO, CaO, SrO, and BaO is in a range from 7 to 12%, and a temperature T 4 at which the glass composition has a viscosity of 10 4 dPa·s is 1080° C. or lower.
- Claim 2Depends on #1
The glass composition according to claim 1 , consisting essentially of, in mass %: 58 to 62% SiO 2 ; 0 to 1% B 2 O 3 ; 8 to 11% Al 2 O 3 ; 7 to 10% MgO; 0 to 0.7% CaO; 18 to 22% Na 2 O; 0 to 2% K 2 O; 0 to 1% TiO 2 ; 0 to 1.5% ZrO 2 ; 0.02% or less total iron oxide in terms of Fe 2 O 3; 0.1 to 0.4% SO 3 ; and 0 to 0.3% SnO 2 , wherein the total content of MgO, CaO, SrO, and BaO is in a range from 7 to 10%.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
References Cited — Backward Prior Art (17)
Non-Patent Literature (1)
- Machine Translation of JP 2013-193887 A, Sep. 30, 2013.