An alloy consists essentially of, in terms of weight percent: 6 to 8.5 Cr, 5.5 to 13.5 Mo, 0.4 to 7.5 W, 1 to 2 Ti, 0.7 to 0.85 Mn, 0.05 to 0.3 Al, up to to 0.1 Co, 0.08 to 0.5 C, 1 to 5 Ta, 1 to 4 Nab, 1 to 3 Hf, balance Ni. The alloy is characterized by, at 850° C., a yield strength of at least 36 Ksi, a tensile strength of at least 40 Ksi, a creep rupture life at 12 Ksi of at least 72.1 hours, and a corrosion rate, expressed in weight loss [g/(cm2sec)]×10 −11 during a 1000 hour immersion in liquid FLiNaK at 850° C., in the range of 8 to 25.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An alloy for use in components in contact with liquid fluorides, consisting essentially of, in terms of weight percent: Cr: 6 to 8.5, Mo: 5.5 to 13.5, W: 0.4 to 7.5, Ti: 1 to 2, Mn: 0.7 to 0.85, Al: 0.05 to 0.3, Co: 0 to 0.1, C: 0.08 to 0.5, Ta: 1 to 5, Nb: 1 to 4, Hf: 1 to 3, Fe: ≦0.01, Ni: balance, with Al+Ti≦2.3 wt. %; and said alloy being characterized by i) at alloy temperatures of 850° C., a yield strength of at least 36 Ksi, a tensile strength of at least 40 Ksi, a creep rupture life at 12 Ksi of at least 72.1 hours, and a corrosion rate of 8×10 −11 g/cm 2 s to 25×10 −11 g/cm 2 s of w
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- "Advanced Sensor System for Energy Infrastructure Assurance", Jan. 2004, Office of Energy Assurance, U.S Department of Energy, 2 pages.
- ASM International, Materials Park, Ohio, Properties and Selection: Nonferrous Alloys and Special Purpose Materials: Nickel and Nickel Alloys, Oct. 1990, vol. 2, pp. 428-445.
- Barner, J.H. Von et al., "Vibrational Spectra of Fluoro and Oxofluoro Complexes of Nb(V) and Ta(V)", Materials Science Forum vols. 73-75 (1991) pp. 279-284 © (1991) Trans Tech Publications, Switzerland doi:10.4028/www.scientific.net/MSF.73-75.279.
- Bruemmer, Stephen M. and Gary S. Was, Microstructural and Microchemical Mechanisms Controlling Intergranular Stress Corrosion Cracking in Light-Water-Reactor Systems, Journal of Nuclear Materials, 1994, pp. 348-363, , vol. 216.
- Delpech et al.: "MSFR: Material Issues and the Effect of Chemistry Control", GIF Symposium, Paris France, Sep. 9-10, 2009.