US 9,673,146 B2#77546339 Most CitedActiveUnited States (USPTO)Utility

Low temperature tungsten film deposition for small critical dimension contacts and interconnects

0Forward Citations (#77546339 Global)
0.0/yrCitation Velocity (#77546339 Global)
0.56Citation PageRank (#77546339 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Provided are methods of void-free tungsten fill of high aspect ratio features. According to various embodiments, the methods involve a reduced temperature chemical vapor deposition (CVD) process to fill the features with tungsten. In certain embodiments, the process temperature is maintained at less than about 350° C. during the chemical vapor deposition to fill the feature. The reduced-temperature CVD tungsten fill provides improved tungsten fill in high aspect ratio features, provides improved barriers to fluorine migration into underlying layers, while achieving similar thin film resistivity as standard CVD fill. Also provided are methods of depositing thin tungsten films having low-resistivity. According to various embodiments, the methods involve performing a reduced temperature low resistivity treatment on a deposited nucleation layer prior to depositing a tungsten bulk layer and/or depositing a bulk layer via a reduced temperature CVD process followed by a high temperature CVD process.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of filling a recessed feature on a substrate, the method comprising: providing a substrate having a field region and a first recessed feature, the first recessed feature being recessed from the field region and comprising sidewalls, a bottom, an opening, and corners; depositing a tungsten nucleation layer on the sidewalls and bottom of the first recessed feature; and filling the first recessed feature with a low temperature CVD tungsten bulk layer via a chemical vapor deposition (CVD) process; wherein the substrate temperature during the CVD process is maintained at between about 250°

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the first recessed feature has an aspect ratio of at least 10:1.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the first recessed feature has an aspect ratio of at least 20:1

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
JP S5629648 AHigh hardness sintered body—23
US 4,746,375 AActivation of refractory metal surfaces for electroless plating198880
US 4,804,560 AMethod of selectively depositing tungsten upon a semiconductor substrate1989123
US 4,874,719 AMethod for manufacturing an electrical connection between conductor levels198995
US 4,962,063 AMultistep planarized chemical vapor deposition process with the use of low melting inorganic material for flowing while depositing1990114
US 5,028,565 AProcess for CVD deposition of tungsten layer on semiconductor wafer1991173
EP 0,437,110 A2Tungsten deposition process for low contact resistivity to silicon—24
US 5,227,329 AMethod of manufacturing semiconductor device1993172
US 5,250,467 AMethod for forming low resistance and low defect density tungsten contacts to silicon semiconductor wafer1993116
US 5,250,329 AMethod of depositing conductive lines on a dielectric199375
US 5,308,655 AProcessing for forming low resistivity titanium nitride films199466
US 5,326,723 AMethod for improving stability of tungsten chemical vapor deposition1994145
US 5,370,739 ARotating susceptor semiconductor wafer processing cluster tool module useful for tungsten CVD1994149
US 5,391,394 ATungsten deposition process for low contact resistivity to silicon1995112
JP H08115984 ASemiconductor device and its manufacture—28
US 5,567,583 AMethods for reducing non-specific priming in DNA detection1996122
JP H0927596 AManufacture of semiconductor device—27
US 5,633,200 AProcess for manufacturing a large grain tungsten nitride film and process for manufacturing a lightly nitrided titanium salicide diffusion barrier with a large grain tungsten nitride cover layer1997135
US 5,661,080 AMethod for fabricating tungsten plug199792
US 5,726,096 AMethod for forming a tungsten silicide layer in a semiconductor device199893
JP H10144688 AMethod of forming contact plugs of semiconductor device having contact holes different in size—29
JP H10163132 AMetal wiring of semiconductor device and its formation—26
US 5,795,824 AMethod for nucleation of CVD tungsten films1998103
US 5,804,249 AMultistep tungsten CVD process with amorphization step1998115
US 5,817,576 AUtilization of SiH4 soak and purge in deposition processes199881
US 5,833,817 AMethod for improving conformity and contact bottom coverage of sputtered titanium nitride barrier layers199848
WO 9,851,838 A1Low resistivity w using b2h¿6?—97
US 5,913,145 AMethod for fabricating thermally stable contacts with a diffusion barrier formed at high temperatures199986
US 5,916,365 ASequential chemical vapor deposition1999819
US 5,916,634 AChemical vapor deposition of W-Si-N and W-B-N199954