US 9,664,997 B2#99485696 Most CitedActiveUnited States (USPTO)Utility

Method of manufacturing mask blank and method of manufacturing transfer mask

0Forward Citations (#99485696 Global)
0.0/yrCitation Velocity (#99485696 Global)
0.56Citation PageRank (#99485696 Global)
16Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Methods of manufacturing a mask blank and a transfer mask that reduce internal stress of a thin film. The methods include preparing a transparent substrate having a pair of opposing main surfaces and composed of a glass material having a hydrogen content of less than 7.4×1018 molecules/cm3, forming a thin film composed of a material containing silicon or metal on one of the main surfaces of the transparent substrate, and carrying out heating treatment or photo irradiation treatment on the transparent substrate with the thin film. The absolute value of a variation of flatness in a predetermined region, as calculated based on a difference in shape obtained from a shape of a main surface of the transparent substrate prior to forming the thin film and a shape of a main surface of the substrate exposed after removing the thin film, is not more than 100 nm.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a mask blank provided with a thin film on a transparent substrate, comprising: a step of preparing a transparent substrate having a pair of opposing main surfaces that is composed of a glass material having a hydrogen content of not more than −2.0×10 17 molecules/cm 3 , a step of forming a thin film composed of a material containing at least one of silicon and metal on one of the main surfaces of the transparent substrate, and a step of carrying out heating treatment or photo irradiation treatment on the transparent substrate on which the thin film has been formed; w

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (16)

PatentTitleYearCitations
JP 2002162726 AMethod of manufacturing phase shift mask blank and phase shift mask—70
US 6,499,317 B1Synthetic quartz glass and method for production thereof200232
US 6,723,477 B2Method for manufacturing phase shift mask blank and method for manufacturing phase shift mask20046
JP 2004199035 AMethod for manufacturing photomask blank and photomask—36
JP 2005298330 ASynthetic quartz glass and its manufacturing method—11
US 7,195,846 B2Methods of manufacturing photomask blank and photomask200713
JP 2007182367 ATitania-doped quartz glass, euv lithographic member and photomask substrate and making method for titania-doped quartz glass—35
JP 2009514774 Aデューテロキシルドープ石英ガラス、このガラスを有する光学部材及びリソグラフィシステム並びにこのガラスの作成方法—10
US 7,585,598 B2Titania-doped quartz glass and making method, EUV lithographic member and photomask substrate200911
US 7,635,658 B2Deuteroxyl-doped silica glass, optical member and lithographic system comprising same and method of making same20091
JP 2010237502 AMethod for inspecting photomask blank or intermediate thereof, method for determining dosage of high-energy radiation, and method for manufacturing photomask blank—9
TW 201,142,486 APhase shift mask blank, manufacturing method thereof, and phase shift mask—1
JP 2012072053 ATitania-doped quartz glass and method for manufacturing the same—11
US 8,168,351 B2Method for inspecting photomask blank or intermediate thereof, method for determining dosage of high-energy radiation, and method for manufacturing photomask blank20121
US 2013071777 A1Phase shift mask blank, method of manufacturing the same, and phase shift mask—11
US 8,820,122 B2Titania-doped quartz glass and making method20146

Non-Patent Literature (2)

  • International Search Report of PCT/JP2013/078861, dated Nov. 26, 2013. [PCT/ISA/210].
  • Notification of Reasons for Refusal dated Dec. 14, 2016, issued by the Taiwan Intellectual Property Office in counterpart Taiwanese Application No. 102139423.