Aluminum alloy wire rod, aluminum alloy stranded wire, coated wire, wire harness and manufacturing method of aluminum alloy wire rod
Abstract
An aluminum alloy wire rod has a composition consisting of 0.1-1.0 mass % Mg; 0.1-1.0 mass % Si; 0.01-1.40 mass % Fe; 0.000-0.100 mass % Ti; 0.000-0.030 mass % B; 0.00-1.00 mass % Cu; 0.00-0.50 mass % Ag; 0.00-0.50 mass % Au; 0.00-1.00 mass % Mn; 0.00-1.00 mass % Cr; 0.00-0.50 mass % Zr; 0.00-0.50 mass % Hf; 0.00-0.50 mass % V; 0.00-0.50 mass % Sc; 0.00-0.50 mass % Co; 0.00-0.50 mass % Ni; and the balance being Al and incidental impurities, wherein at least one or none of Ti, B, Cu, Ag, Au, Mn, Cr, Zr, —Hf, V, Sc, Co and Ni is contained in the composition. A dispersion density of an Mg 2 Si compound having a particle size of 0.5 μm to 5.0 μm is less than or equal to 3.0×10 −3 particles/μm 2 . In a sectional structure, a concentration of each of Si and Mg other than a compound is less than or equal to 2.00 mass %.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An aluminum alloy wire rod having a composition consisting of 0.1 mass % to 1.0 mass % Mg; 0.1 mass % to 1.0 mass % Si; 0.01 mass % to 1.40 mass % Fe; 0.000 mass % to 0.100 mass % Ti; 0.000 mass % to 0.030 mass % B; 0.00 mass % to 1.00 mass % Cu; 0.00 mass % to 0.50 mass % Ag; 0.00 mass % to 0.50 mass % Au; 0.00 mass % to 1.00 mass % Mn; 0.00 mass % to 1.00 mass % Cr; 0.00 mass % to 0.50 mass % Zr; 0.00 mass % to 0.50 mass % Hf; 0.00 mass % to 0.50 mass % V; 0.00 mass % to 0.50 mass % Sc; 0.00 mass % to 0.50 mass % Co; 0.00 mass % to 0.50 mass % Ni; and the balance being Al and incidental impu
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (22)
Non-Patent Literature (5)
- Chinese Office Action and Search Report for Chinese Application No. 201380053482.0, dated Aug. 26, 2016, with an English translation thereof.
- Decision to Grant a Patent of Japanese Patent Application No. 2014-508615, mailed Aug. 11, 2014.
- Extended European Search Report for counterpart European Application No. 13879835.0, mailed Jul. 4, 2016.
- International Preliminary Report on Patentability and Written Opinion of the International Searching Authority (Forms PCT/IB/373 and PCT/ISA/237) for International Application No. PCT/JP2013/080955, dated Sep. 29, 2015, with an English translation.
- International Search Report, mailed Feb. 4, 2014, issued in PCT/JP2013/080955.