Patents
US 9,640,433 B2#101936259 Most CitedActiveUnited States (USPTO)Utility

Methods of forming interconnects and semiconductor structures

0Forward Citations (#101936259 Global)
0.0/yrCitation Velocity (#101936259 Global)
0.56Citation PageRank (#101936259 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method of activating a metal structure on an intermediate semiconductor device structure toward metal plating. The method comprises providing an intermediate semiconductor device structure comprising at least one first metal structure and at least one second metal structure on a semiconductor substrate. The at least one first metal structure comprises at least one aluminum structure, at least one copper structure, or at least one structure comprising a mixture of aluminum and copper and the at least one second metal structure comprises at least one tungsten structure. One of the at least one first metal structure and the at least one second metal structure is activated toward metal plating without activating the other of the at least one first metal structure and the at least one second metal structure. An intermediate semiconductor device structure is also disclosed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of forming a semiconductor structure, comprising: selectively forming nickel over a tungsten material on a substrate without forming the nickel over one or more of an aluminum material and a copper material on the substrate; activating the aluminum material or the copper material to nickel plating; and forming nickel over an exposed surface of the aluminum material or the copper material.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein selectively forming nickel over a tungsten material on a substrate without forming the nickel over one or more of an aluminum material and a copper material comprises: exposing the substrate to a palladium(II) solution to activate the tungsten material without activating the aluminum material or the copper material; and exposing the substrate to a nickel plating solution.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,726,771 AProcess for chemical nickel plating of aluminum and its alloys197323
US 4,017,265 AFerromagnetic memory layer, methods of making and adhering it to substrates, magnetic tapes, and other products197730
US 4,104,111 AProcess for manufacturing printed circuit boards197873
US 4,125,648 AElectroless deposition of nickel on aluminum197827
EP 0,455,915 A1Electroless plating of nickel onto surfaces such as copper or fused tungsten—9
US 5,079,040 AProcess for electrolessly depositing nickel199224
US 5,147,692 AElectroless plating of nickel onto surfaces such as copper or fused tungston199270
US 5,169,680 AElectroless deposition for IC fabrication1992184
US 5,580,668 AAluminum-palladium alloy for initiation of electroless plating199634
US 5,608,264 ASurface mountable integrated circuit with conductive vias1997305
US 5,618,752 AMethod of fabrication of surface mountable integrated circuits1997286
US 5,646,067 AMethod of bonding wafers having vias including conductive material1997272
US 5,682,062 ASystem for interconnecting stacked integrated circuits1997350
US 5,795,619 ASolder bump fabricated method incorporate with electroless deposit and dip solder199826
US 5,814,889 AIntergrated circuit with coaxial isolation and method1998310
US 6,028,011 AMethod of forming electric pad of semiconductor device and method of forming solder bump2000113
US 6,083,834 AZincate catalysis electroless metal deposition for via metal interconnection200011
US 2001002317 A1Methods of forming materials comprising tungsten and nitrogen, and methods of forming capacitors—11
US 6,261,367 B1Method and apparatus for dispensing liquid material200141
US 6,300,678 B1I/O pin having solder dam for connecting substrates200156
US 2001036746 A1Methods of producing and polishing semiconductor device and polishing apparatus—68
US 6,346,148 B1Apparatus for coating a moving web with at least two coat layers200213
US 2002043466 A1Method and apparatus for patching electrochemically deposited layers using electroless deposited materials—33
US 2002047210 A1Semiconductor chip, wiring board and manufacturing process thereof as well as semiconductor device—83
US 6,407,570 B1Interconnect for testing semiconductor components having support members for preventing component flexure200216
US 6,452,274 B1Semiconductor device having a low dielectric layer as an interlayer insulating layer200273
US 6,458,696 B1Plated through hole interconnections200291
US 6,479,902 B1Semiconductor catalytic layer and atomic layer deposition thereof200242
US 2002190371 A1Semiconductor device and method of production of same—56
US 6,503,343 B1Controlled plating on reactive metals200340

Non-Patent Literature (5)

  • International Preliminary Report on Patentability for International Application No. PCT/US2005/030228 dated Jul. 31, 2007, 11 pages.
  • International Search Report for International Application No. PCT/US2005/030228 dated Jul. 12, 2007, 6 pages.
  • International Written Opinion for International Application No. PCT/US2005/030228 dated Jul. 12, 2007, 10 pages.
  • Law et al., "The Effect of Passivation Defect on Electroless Nickel Under Bump Metallization Plating Process," www.ee.vst.hk/˜flipchip/ctu-simon.doc.
  • Law et al., “The Effect of Passivation Defect on Electroless Nickel Under Bump Metallization Plating Process,” www.ee.vst.hk/˜flipchip/ctu—simon.doc.