To provide a price-competitive compression ring having excellent thermal conductivity and thermal sag resistance, which can be used in a high-thermal-load environment of high-compression-ratio engines, steel identified by the material number of SUP10 in JIS G 4801, which contains small amounts of alloying elements, is used, and a piston ring wire is annealed before an oil-tempering treatment such that spheroidal cementite having an average particle size of 0.1-1.5 μm is dispersed in a tempered martensite matrix, thereby suppressing the movement of dislocation and creep even at 300° C., and improving thermal sag resistance.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 31 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A compression ring consisting of a composition consisting of by mass 0.45-0.55% of C, 0.15-0.35% of Si, 0.65-0.95% of Mn, 0.80-1.10% of Cr, and 0.15-0.25% of V, the balance being Fe and inevitable impurities, and spheroidal cementite having an average particle size of 0.1-1.5 μm dispersed in a tempered martensite matrix, wherein said compression ring has thermal conductivity of 35 W/m·K or more and thermal sag ratio of 4.4% or less.

  2. Claim 2Depends on #1

    The compression ring according to claim 1 , wherein the amount of said spheroidal cementite dispersed is 1-6% by area on a microscopically observed structure surface.

  3. Claim 3Depends on #1

    The compression ring according to claim 1 , having a thermal conductivity of 38 W/m·K or more, and thermal sag ratio of 4% or less.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (31)

PatentTitleYearCitations
JP S5845357 AMaterial for piston ring—12
JP S63223147 APiston ring material—17
US 4,966,751 ASteel having good wear resistance199053
JP H06299296 ASteel for high strength spring excellent in decarburizing resistance—6
JP 2000239797 ASteel for spring excellent in workability and production of steel wire for spring—17
JP 2000337511 APiston-ring abrasion-resistant ring made of free-graphite precipitated iron system sintered material excellent in abrasion resistance and heat conductivity—21
WO 0,148,258 A1Bar or wire product for use in cold forging and method for producing the same—6
US 6,306,230 B1Process for the production of hardened parts of steel200112
JP 2001294989 AWear resistant steel and piston ping or liner material of internal combustion engine—10
US 6,372,056 B1Spring steel superior in workability200234
US 2003075250 A1Bar or wire product for use in cold forging and method for producing the same—13
US 6,602,359 B1Bar or wire product for use in cold forging and method for producing the same200328
US 2004047757 A1High-hardness, high-toughness steels and crawler components, earth wear resistant components, fastening bolts, high-toughness gears, high-toughness, high contact pressure resistance gears, and wear resistant steel plates using the same—68
US 2004256029 A1Rolling element and method of producing the same—22
US 2005103777 A1Gear part and method of producing thereof—7
JP 2006183137 ASteel wire for high strength spring—70
US 2006219054 A1Wear resistant sintered member and production method therefor—14
JP 2007321199 ASteel for piston ring excellent in seizure resistance, deformed wire for piston ring, and piston ring—9
EP 1,887,096 A1Hot working steel—18
US 2008279714 A1High Strength Spring Steel and Steel Wire—31
KR 20090071164 AHigh-strength steel bolt having excellent resistance for delayed fracture and notch toughness method for producing the same—11
WO 2009/093527 A1Alloy to be surface-coated and sliding members—2
US 7,575,619 B2Wear resistant sintered member20099
US 2009226756 A1Piston ring—17
JP 2009235561 APiston ring—24
US 2009277539 A1Steel for Warm Working, Warm Working Method Using the Steel, and Steel Material and Steel Component Obtainable Therefrom—28
US 2010189592 A1Process for Setting the Thermal Conductivity of a Steel, Tool Steel, in Particular Hot-Work Steel, and Steel Object—14
US 2010291407 A1Alloy to be surface-coated and sliding members—1
US 8,409,712 B2Alloy to be surface-coated and sliding members20131
US 8,557,056 B2Process for setting the thermal conductivity of a steel, tool steel, in particular hot-work steel, and steel object20135

Non-Patent Literature (5)

  • "Cast steel: The Formation of Martensite." Key to Metals. Web. Aug. 13, 2009.
  • "The Tempering of Martensite: Part One." Key to Metals. Web. Feb. 17, 2009.
  • G. F. Carter, D. E. Paul. "Materials Science and Engineering." ASM International, 1991, p. 104, Fig. 6.1.
  • International Search Report issued in PCT/JP2011/061857, mailed on Jul. 12, 2011.
  • Japanese Office Action, dated Feb. 18, 2014, for Japanese Application No. 2010-119048 with an English translation.