Patents
US 9,617,629 B2#60951033 Most CitedActiveUnited States (USPTO)Utility

Copper-nickel-zinc alloy containing silicon

1Forward Citations (#60951033 Global)
0.1/yrCitation Velocity (#44869682 Global)
0.76Citation PageRank (#60951033 Global)
22Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention includes a copper-nickel-zinc alloy with the following composition in weight %: Cu 47.0 to 49.0%, Ni 8.0 to 10.0%, Mn 0.2 to 0.6%, Si 0.05 to 0.4%, Pb 1.0 to 1.5%, Fe and/or Co up to 0.8%, the rest being Zn and unavoidable impurities, wherein the total of the Fe content and double the Co content is at least 0.1 weight % and wherein mixing silicides containing nickel, iron and manganese and/or containing nickel, cobalt and manganese are stored as spherical or ellipsoidal particles in a structure consisting of an α- and β-phase. The invention further relates to a method for producing semi-finished products from a copper-nickel-zinc alloy.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A copper-nickel-zinc alloy having the following composition, in % by weight: Cu 47.0 to 49.0%, Ni 8.0 to 10.0%, Mn 0.2 to 0.6%, Si 0.05 to 0.4%, Pb 1.0 to 1.5%, Fe and/or Co up to 0.8%, remainder Zn and unavoidable impurities, wherein a sum total of the Fe content and twice the Co content is at least 0.1%, mixed silicides containing nickel, iron and manganese and/or mixed silicides containing nickel, cobalt and manganese are incorporated as spherical or ellipsoidal particles in a microstructure consisting of α and β phase and an areal density of the silicides having a particle diameter of at m

  2. Claim 2Depends on #1

    The copper-nickel-zinc alloy as claimed in claim 1 , characterized in that either the Fe content or the Co content is at least 0.1% by weight.

  3. Claim 3Independent Claim

    The c

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (22)

PatentTitleYearCitations
DE 1,120,151 BHochfeste Neusilber-Legierung—16
DE 1,205,285 BVerwendung von mangan- und siliziumhaltigen Kupferlegierungen fuer auf Abnutzung beanspruchte Gegenstaende—10
DE 1,238,220 BVerwendung einer Kupfer-Mangan-Zink-Legierung als Werkstoff fuer einer Gleitbeanspruchung ausgesetzte Maschinenteile—8
DE 1,558,817 A1Verfahren zur Herstellung von Halbzeugen oder Halbfabrikaten aus Kupferlegierungen mit beta- und alpha-Gefuege—21
US 3,627,593 ATwo phase nickel-zinc alloy19718
US 4,631,171 ACopper-zinc-manganese-nickel alloys198617
US 4,684,052 AMethod of brazing carbide using copper-zinc-manganese-nickel alloys198740
JP H01116044 AUse of copper-zinc alloy—8
JP H01177327 AFree cutting copper-based alloy showing silver-white—33
US 4,954,187 APrecipitates copper-zinc alloy with nickel silicide199019
EP 0,222,004 B1Copper-zinc-manganese-nickel alloys19908
JP H0368732 AManufacture of copper alloy and copper alloy material for radiator plate—12
DE 4,339,426 A1Kupfer-Zink-Legierung—3
JP H07166279 ACopper-base alloy excellent in corrosion resistance, punchability, and machinability and production thereof—24
JP H07216493 ACopper - zinc alloy—4
US 5,658,401 ACopper-zinc alloy199729
US 2006065336 A1Copper-based alloy—14
EP 1,608,789 B1Copper-based alloy200712
DE 102007029991 A1Copper-zinc-alloy, useful e.g. for producing pipes and rods, comprises zinc, silicon, manganese, nickel, aluminum, iron, optionally lead, tin, phosphorus and sulfur and the rest of copper and unavoidable impurities stored in matrix—15
US 2009022620 A1Copper-zinc alloy, production method and use—49
CH 700,999 A2Copper-nickel-zinc alloy comprises copper, nickel, manganese, silicon, optionally aluminum and lead, zinc and impurities, where a silicide e.g. manganese-nickel silicide, is embedded in a two-phase microstructure—8
DE 102009021336 A1Kupfer-Nickel-Zink-Legierung und deren Verwendung—17

Non-Patent Literature (3)

  • Form PCT/ISA/210 International Search Report issued in International Application No. PCT/EP2013/000373 with English translation of categories of documents cited dated May 19, 2014 (3 pages).
  • Japanese Office Action mailed Jul. 28, 2015 and a partial English translation thereof (7 pgs.).
  • Office Action of German Patent Office issued in Application No. 10 2012 004 725.8 dated Dec. 4, 2012 (6 pages).