Molten-salt bath for nitriding mechanical parts made of steel, and implementation method
Abstract
A molten-salt bath for nitriding mechanical steel parts, essentially consisting of the following (the contents being expressed in wt %): 25 to 60 wt % of alkali-metal chlorides; 10 to 40 wt % of alkali-metal carbonates; 20 to 50 wt % of alkali-metal cyanates; and a maximum of 3 wt % of cyanide ions (formed during the use of the bath), wherein the total of the contents is 100 wt %. Preferably, the bath contains: 25 to 30 wt % of sodium cyanate; 25 to 30 wt % of sodium carbonate and lithium carbonate; 40 to 50 wt % of potassium chlorides; and a maximum of 3 wt % of cyanide ions (formed during the use of the bath), the total of the contents being 100 wt %.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
Molten-salt bath for nitriding mechanical parts made of steel, consisting essentially of by weight: 40% to 60% alkali metal chlorides selected from the group consisting of lithium, sodium and potassium chlorides, 10% to 40% alkali metal carbonates, 20% to 40% alkali metal cyanates, and a maximum of 3% cyanide ions.
- Claim 2Depends on #1
The molten-salt bath according to claim 1 , wherein the content of alkali metal chloride is between 40% and 50%.
- Claim 3Depends on #1
The molten-salt bath according to claim 1 , wherein the content of alkali metal chloride is 43-47%.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (18)
Non-Patent Literature (1)
- International Search Report, dated May 7, 2012, from corresponding PCT application.