Patents
US 9,608,263 B2#136646920 Most CitedActiveUnited States (USPTO)Utility

Anode material having a uniform metal-semiconductor alloy layer

0Forward Citations (#136646920 Global)
0.0/yrCitation Velocity (#136646920 Global)
0.56Citation PageRank (#136646920 Global)
24Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to methods for producing anode materials for use in nonaqueous electrolyte secondary batteries. In the present invention, a metal-semiconductor alloy layer is formed on an anode material by contacting a portion of the anode material with a solution containing metals ions and a dissolution component. When the anode material is contacted with the solution, the dissolution component dissolves a part of the semiconductor material in the anode material and deposit the metal on the anode material. After deposition, the anode material and metal are annealed to form a uniform metal-semiconductor alloy layer. The anode material of the present invention can be in a monolithic form or a particle form. When the anode material is in a particle form, the particulate anode material can be further shaped and sintered to agglomerate the particulate anode material.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A secondary battery comprising an anode, a cathode and a non aqueous electrolyte, the anode comprising a porous agglomerated mass of a sintered particulate material, wherein the particulate material comprises a semiconductor material core and a metal-semiconductor alloy layer thereon and has a diameter of about 0.001 micrometers to 100 micrometers, the volume of the metal-semiconductor alloy layer is about 0.1% to 5% of the total particle volume; and wherein particles within the agglomerated mass are adhered together by the metal-semiconductor alloy layer.

  2. Claim 2Depends on #1

    The secondary battery of claim 1 wherein the semiconductor material comprises silicon or germanium.

  3. Claim 3Depends on #2

    The secondary battery of claim 2 wherein the metal of the metal-semiconductor alloy is nickel, copper, cobalt, silver, gold, platinum, palladium or rh

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
EP 0,883,199 A1Negative electrode materials for non-aqueous electrolyte secondary batteries and said batteries employing the same materials—88
US 6,090,505 ANegative electrode materials for non-aqueous electrolyte secondary batteries and said batteries employing the same materials2000158
EP 1,028,476 A1Negative electrode material for nonaqueous electrode secondary battery and method for producing the same—101
CN 1,286,811 ANegative electrode material for nonaqueous electrode secondary battery and method for producing same—57
EP 1,100,134 A1Nonaqueous electrolyte secondary cell and its negative plate—59
US 6,235,427 B1Nonaqueous secondary battery containing silicic material2001364
EP 1,102,340 A2Methods of manufacturing negative material and secondary battery—52
US 6,287,371 B1Non-electrolytic gold plating liquid and non-electrolytic gold plating method using same200159
US 6,432,579 B1Method of manufacturing secondary battery negative electrode2002164
US 6,525,391 B1Nickel silicide process using starved silicon diffusion barrier200351
US 2003175589 A1Process for manufacture of negative electrode material for a non-aqueous electrolyte secondary battery—88
US 6,679,925 B1Methods of manufacturing negative material and secondary battery200454
US 2004234861 A1Electrode and battery using it—64
US 2005095503 A1Battery—68
US 2005130383 A1Silicide resistor in beol layer of semiconductor device and method—38
US 2007031733 A1Lithium secondary battery—72
US 2009029256 A1Si/c composite, anode active materials, and lithium battery including the same—141
US 2009263716 A1Anode material having a uniform metal-semiconductor alloy layer—19
WO 2009/129490 A1Anode material having a uniform metal-semiconductor alloy layer—18
EP 2,277,214 A1Anode material having a uniform metal-semiconductor alloy layer—3
US 8,133,613 B2Nonaqueous electrolyte secondary battery anode material with a uniform metal-semiconductor alloy layer20122
US 8,367,244 B2Anode material having a uniform metal-semiconductor alloy layer20134
US 8,524,395 B2Nonaqueous electrolyte secondary battery anode material with a uniform metal-semiconductor alloy layer20131
US 9,105,905 B2Anode material having a uniform metal-semiconductor alloy layer20153

Non-Patent Literature (5)

  • Broussely et al., Li-ion batteries and portable power source prospects for the next 5-10 years, Journal of Power Sources, 136, 2004, 386-394.
  • Dierks, S., GuideChem, NickelSilicide (Ni2Si) (cas 12059-14-2) MSDS, Material safety data sheet, retrieved from www.guidechem.com/cas-120/12059-14-2.html, 2 pgs. Sep. 30, 1993.
  • Golodnitsky et al., Advanced materials for the 3D microbattery, Journal of Power Sources, 2006, 153, 281-287.
  • Harraz et al., Different behavior in immersion plating of nickel on porous silicon from acidic and and alkaline fluoride media, J. Elect. Soc., 2003, 150(5): C277-284.
  • Harraz et al., Immersion plating of nickel onto a porous silicon layer from fluoride solutions, Phys. Stat. Sol., 2003, 197(1): 51-56.