Patents
US 9,605,329 B2#16029476 Most CitedActiveUnited States (USPTO)Utility

Cold rolled steel sheet and manufacturing method thereof

7Forward Citations (#16029476 Global)
0.8/yrCitation Velocity (#9658407 Global)
1.39Citation PageRank (#25626936 Global)
37Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

When the amount of C, the amount of Si and the amount of Mn are respectively represented by [C], [Si] and [Mn] in unit mass %, the cold rolled steel sheet satisfies a relationship of (5×[Si]+[Mn])/[C]>10, the metallographic structure contains, by area ratio, 40% to 90% of a ferrite and 10% to 60% of a martensite, further contains one or more of 10% or less of a pearlite by area ratio, 5% or less of a retained austenite by volume ratio and 20% or less of a bainite by area ratio, the hardness of the martensite measured using a nanoindenter satisfies H20/H10<1.10 and σHM0<20, and TS×λ representing the product of TS that is a tensile strength and λ that is a hole expansion ratio is 50000 MPa·% or more.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 37 · Forward citations: 7.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A cold rolled steel sheet comprising, by mass %: C: more than 0.150% to 0.300%; Si: 0.010% to 1.000%; Mn: 1.50% to 2.70%; P: 0.001% to 0.060%; S: 0.001% to 0.010%; N: 0.0005% to 0.0100%; and Al: 0.010% to 0.050%, and optionally one or more of: B: 0.0005% to 0.0020%; Mo: 0.01% to 0.50%; Cr: 0.01% to 0.50%; V: 0.001% to 0.100%; Ti: 0.001% to 0.100%; Nb: 0.001% to 0.050%; Ni: 0.01% to 1.00%; Cu: 0.01% to 1.00%; Ca: 0.0005% to 0.0050%; and REM: 0.0005% to 0.0050%, and a balance including Fe and unavoidable impurities, wherein, when an amount of C, an amount of Si and an amount of Mn are respective

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (37)

PatentTitleYearCitations
JP H01172524 AProduction of complex phase structure chromium stainless strip having excellent corrosion resistance and high ductility and strength—33
JP H06128688 AHot rolled steel plate excellent in fatigue characteristic and it production—34
JP H11189842 AHigh-strength and high-workability hot rolled steel plate excellent in impact resistance, balance between strength and elongation, fatigue resistance, and bore-expandability, and its production—25
JP 2000319756 AHot rolled steel sheet for working excellent in fatigue characteristic and its production—25
JP 2001355044 AHigh strength steel sheet excellent in formability and hole expansibility, and its production method—32
JP 2003193192 AHigh strength steel sheet having excellent formability and chemical convertibility and production method therefor—10
JP 2003313636 AHot-dipped steel sheet with high ductility and high strength, and manufacturing method therefor—19
JP 2004018912 AHigh-tensile strength cold-rolled steel plate excellent in elongation and stretch-flanging property and method for manufacturing the same—17
JP 2005120436 AHigh-strength steel sheet superior in hole-expandability and ductility, and manufacturing method therefor—29
JP 2005256141 AMethod for manufacturing high-strength steel sheet superior in hole expandability—23
US 2007023113 A1Dual-phase steel sheet excellent in stretch flange formability and production method thereof—21
JP 2007314817 ASteel sheet to be hot-pressed, hot-pressed steel sheet member, and method for manufacturing them—146
RU 2,312,162 C2High-strength steel sheet with molten zinc coat and method of manufacture of such sheet200743
RU 2,312,920 C2Alloyed steel sheet with molten zinc coat and method of manufacture of such sheet200720
JP 2008156734 AHigh-strength hot-dip galvanized steel sheet and its manufacturing method—67
EP 2,128,295 A1High-strength hot dip zinc plated steel sheet having excellent moldability, and method for production thereof—33
RU 2,379,373 C1Manufacturing method of detail with quite high mechanical strength from rolled sheet with coating201010
JP 2010065292 AHot press member having excellent ductility, steel sheet for the hot press member and method for producing the hot press member—74
RU 2,395,593 C1Coated steel strips, methods of their fabrication and application, pressed billets made thereof, pressed products made thereof and industrial products comprising such pressed products201030
CN 101,802,233 ADual phase steel, by the flat product of this dual phase steel preparation and the method for preparing flat product—38
RU 2,403,311 C2Manufacturing method of high-strength steel plates with excellent ductility and plates made by means of this method201012
EP 2,264,206 A1High-strength steel sheets which are extremely excellent in the balance between burring workability and ductility and excellent in fatigue endurance, zinc-coated steel sheets, and processes for production of both—22
CN 101,939,457 AHigh strength galvanized steel sheet with excellent formability and method for manufacturing the same—13

Non-Patent Literature (5)

  • Canadian Office Action dated Jun. 28, 2016, issued in Canadian Patent Application No. 2,862,810.
  • International Search Report dated Apr. 16, 2013 issued in corresponding PCT Application No. PCT/JP2013/050382 [with English Translation].
  • International Search Report dated Apr. 16, 2013 issued in PCT Application No. PCT/JP2013/050377 [with English Translation].
  • Machine-English translation of JP2008-156734, Kawabe Hidenao et al., Jul. 10, 2008.
  • Notice of Allowance issued on Nov. 27, 2015 in corresponding RU Application No. 2014129326.