US 9,601,768 B2#40407253 Most CitedActiveUnited States (USPTO)Utility

Silicon oxide and method of preparing the same

2Forward Citations (#40407253 Global)
0.2/yrCitation Velocity (#31623857 Global)
1.00Citation PageRank (#41565799 Global)
19Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a method of preparing silicon oxide, in which the amounts of silicon and oxygen are appropriately controlled by decreasing the amount of the oxygen from silicon oxide containing a relatively large amount of oxygen, silicon oxide prepared by the method, and a secondary battery including the same. According to the method of preparing silicon oxide, silicon oxide (first silicon oxide) including a relatively large amount of oxygen is heat treated in a reducing atmosphere to decrease the amount of the oxygen in the silicon oxide (first silicon oxide) and to prepare silicon oxide (second silicon oxide) including silicon and oxygen in an appropriate amount (Si:SiO 2 =1:0.7-0.98), thereby improving capacity and initial efficiency and securing stability and cycle properties (lifetime characteristics) of the secondary battery.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 2.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of preparing silicon oxide for anode active material, comprising: providing a first silicon oxide in a reactor in a reaction chamber, and heat treating under a reducing atmosphere to prepare a second silicon oxide, wherein the first silicon oxide is SiO x (0<x<2), and the second silicon oxide is SiO y , where y<x and 0.7<y<0.98, wherein the heat treating is performed at a temperature ranging from 800 ° C. to 1,000 ° C. and the temperature is maintained for 10 to 20 hours, and wherein a crystal size of silicon (Si) in the second silicon oxide is in a range of 0.2 nm to 5

  2. Claim 2Depends on #1

    The method of preparing silicon oxide for anode active material of claim 1 , wherein SiO x in the first silicon oxide satisfies 0.9<x<1.5.

  3. Claim 3Independent Claim

    The method of preparing silicon oxide for anode ac

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (19)

PatentTitleYearCitations
US 4,838,914 AProcess for producing silica glass fibers198916
US 2005048369 A1Negative electrode for non-aqueous electrolyte secondary battery, production method thereof and non-aqueous electrolyte secondary battery—40
EP 1,806,317 A1PROCESS FOR PRODUCING SiOx PARTICLE—3
US 2007207381 A1Negative-electrode active material for nonaqueous electrolyte secondary battery, and negative electrode and nonaqueous electrolyte secondary battery using the same—32
US 2007248525 A1Method for producing silicon oxide powder—9
KR 20070104848 AMethod for producing silicon oxide powder—5
CN 101,381,083 AMethod for preparing high pure spherical silica by means of vacuum carbothermal reduction—16
US 2010243951 A1Negative electrode material for nonaqueous electrolyte secondary battery, making method and lithium ion secondary battery—45
JP 2010225494 AAnode material for nonaqueous electrolyte secondary battery, its manufacturing method, and lithium ion secondary battery—40
JP 2010272411 ANegative electrode material for nonaqueous electrolyte secondary battery and method for manufacturing the negative electrode material, lithium ion secondary battery, and electrochemical capacitor—27
US 2011086271 A1Negative active material for rechargeable lithium battery, method of preparing the same, and rechargeable lithium battery including the same—40
KR 20110040478 ANegative active material for lithium secondary battery, preparing method of the same, and lithium secondary battery including the same—25
JP 2011108635 ANegative electrode active material for lithium ion secondary battery—11
US 7,955,581 B2Method of producing silicon oxide, negative electrode active material for lithium ion secondary battery and lithium ion secondary battery using the same20118
JP 2011142021 ASilicon oxide for nonaqueous electrolyte secondary battery anode material, method of manufacturing silicon oxide for nonaqueous electrolyte secondary battery anode material, lithium ion secondary battery, and electrochemical capacitor—53
US 2011287313 A1Silicon oxide material for nonaqueous electrolyte secondary battery negative electrode material, making method, negative electrode, lithium ion secondary battery, and electrochemical capacitor—29
KR 20120089073 APreparation method of silicon oxide powder using thermal plasma, and the silicon oxide powder thereby—14
US 2012211695 A1Negative electrode active material for lithium-ion secondary battery—2
EP 2,492,995 A1Negative electrode active material for lithium ion secondary battery—2

Non-Patent Literature (1)

  • Office Action of Japanese Patent Office in Appl'n. No. 2014-550230, dated Jun. 30, 2015.