Patents
US 9,592,575 B2#61502567 Most CitedActiveUnited States (USPTO)Utility

Weld metal having excellent resistance to hydrogen embrittlement susceptibility

1Forward Citations (#61502567 Global)
0.1/yrCitation Velocity (#44900000 Global)
0.75Citation PageRank (#61502567 Global)
22Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The weld metal of the present invention is formed by gas shield arc welding using a flux-cored wire, has a predetermined chemical component composition, and contains 20% or more of Ti. The amount of Ti-containing oxide particles having a circle-equivalent diameter of 0.15-1.0 μm is at least 5000 per square mm, the amount of V per total mass of weld metal present as a compound within the weld metal is 0.002% or more, and the average circle equivalent diameter of V-containing carbide present in the weld metal is 15 nm or less.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 1.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A weld metal comprising; C: 0.02 to 0.12% (means “mass %” which is identical here and hereinafter for the chemical component composition), Si: 0.1 to 0.80%, Mn: 0.9 to 2.5%, Ni: 0.20 to 3.5%, Mo: 0.05 to 1.50%, Ti: 0.040 to 0.15%, V: 0.05 to 0.60%, N: 0.015% or less, not including 0%, and O: 0.030% or more respectively, with the balance of iron and unavoidable impurities, wherein Ti-containing oxide particles containing Ti by 20% or more, and having a circle equivalent diameter of 0.15 to 1.0 μm are present by the number of 5,000/mm 2 or more, and the amount of V per total mass of the weld me

  2. Claim 2Depends on #1

    The weld metal of claim 1 , further cont

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (22)

PatentTitleYearCitations
JP H08257785 AFlux cored wire for arc welding to improve low temp. crack resistance of steel weld zone—26
JP H11147196 AShielded metal arc welding method for high tensile strength steel—14
US 6,264,760 B1Ultra-high strength, weldable steels with excellent ultra-low temperature toughness200162
JP 3,208,556 B2アーク溶接用フラックス入りワイヤ20012
JP 2001348649 AWelded joint—4
US 2002026969 A1Heavy wall steel material having superior weldability and method for producing the same—4
JP 2004315962 AHigh strength weld metal having excellent low temperature toughness—20
EP 1,500,457 A1Method for producing an ultrahigh strength welded steel pipe excellent in cold cracking resistance of weld metal—15
US 2005016980 A1Ultrahigh strength welded joint and ultrahigh strength welded steel pipe excellent in cold cracking resistance of weld metal, and methods for producing the same—15
JP 2005040816 AUltrahigh strength weld joint excellent in low temperature cracking property of weld metal, ultrahigh strength welded steel pipe, and their manufacturing methods—28
CN 1,811,000 AHigh-strength spring steel having excellent hydrogen embrittlement resistance—20
JP 2008087043 AGas shielded arc welding flux-cored wire for high-tension steel—23
WO 2010/055788 A1Welded metal—7
JP 2010115701 AHigh strength weld metal with excellent low-temperature toughness—9
WO 2010/110387 A1Weld metal and weld structure having weld joints using the same—6
JP 2010274304 AFlux-cored wire for high-tensile strength steel—34
CN 101,918,607 AHigh strength steel plate for high heat input welding having welded joint with superior impact toughness in weld heat affected zone—10
JP 2011000626 AWeld metal—8
US 2011250471 A1Ultrahigh strength welded joint and ultrahigh strength welded steel pipe excellent in cold cracking resistance of weld metal, and methods for producing the same—6
US 2012021246 A1Weld metal and welded structure having weld joints using the same—8
US 2013315777 A1Weld metal excellent in hydrogen embrittlement resistance—9
EP 2,671,668 A1Weld metal having excellent sensitivity to hydrogen embrittlement resistance—6

Non-Patent Literature (3)

  • English translation of Written Opinion issued Jun. 19, 2012 in PCT/JP12/59599/ Filed Apr. 6, 2012.
  • Extended European Search Report issued on Jul. 28, 2014 in Patent Application No. 12767441.4.
  • International Search Report Issued Jun. 19, 2012 in PCT/JP212/059599 Filed Apr. 6, 2012.