Polyurethane composites produced by a vacuum infusion process
Abstract
A polyurethane-forming system having a viscosity at 25° C. of less than 600 mPas for at least 30 minutes, a gel time at ambient temperature of greater than 60 minutes and a water content of less than 0.06% by weight, based on total system weight, is used to produce composites by a vacuum infusion process. This system makes it possible to produce large composites such as wind turbine blades having excellent physical properties.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing a fiber-reinforced polyurethane composite article by vacuum infusion molding, comprising: (a) degassing components comprising an isocyanate component and an isocyanate-reactive component, wherein: (1) the isocyanate component has a viscosity at 25° C. of from about 20 to about 300 mPas and comprises a diisocyanate or a polyisocyanate, and (2) the isocyanate-reactive component comprises: (i) one or more polyols having a viscosity at 25° C. of from 20 to 850 mPas, and an OH number of from about 200 to about 600, (ii) up to about 6% by weight, based on total isocyanate-rea
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗