Patents
US 9,566,618 B2#45300626 Most CitedActiveUnited States (USPTO)Utility

Silicon sputtering target with special surface treatment and good particle performance and methods of making the same

2Forward Citations (#45300626 Global)
0.2/yrCitation Velocity (#31908014 Global)
0.87Citation PageRank (#49719427 Global)
50Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A sputter target assembly comprising a Si target and a backing plate is provided wherein the backing plate is bonded to the target. The Si target comprises a smooth, mirror-like surface and has a surface roughness of less than about 15.0 Angstroms. Methods are provided for producing silicon target/backing plate assemblies wherein a silicon blank is processed to remove scratches from the blank surface resulting in a mirror like surface on the target, and a surface roughness of 15.0 Angstroms or less. The method comprises a first and second cleaning step with the first step being performed before the scratch removal step, and the second step being performed after the scratch removal.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    Method of cleaning a silicon target comprising providing a Si blank, removing scratches from a surface of said blank so as to provide a mirror surface on said blank having a surface roughness of 15.0 Angstroms or less, said method further comprising a first and second cleaning step, said first cleaning step being performed before said scratch removal and said second step being performed after said scratch removal, wherein either said first or second cleaning steps comprise contacting said blank surface with a liquid cleaning solution comprising a polymer.

  2. Claim 2Independent Claim

    Method of cleaning a silicon target comprising providing a Si blank, removing scratches from a surface of said blank so as to provide a mirror surface on said blank having a surface roughness of 15.0 Angstroms or less, said method further comprising a first and second cleani

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,978,437 AMethod of applying optical coatings of silicon compounds by cathode sputtering, and a sputtering cathode for the practice of the method199064
JP H03261697 ASilicon sputtering system—3
WO 9,217,622 A1Thermally compatible sputter target and backing plate assembly—21
US 5,230,459 AMethod of bonding a sputter target-backing plate assembly assemblies produced thereby1993114
JP H0653137 AFormation of amorphous silicon hydride film—12
JP H06346215 AJoining of silicon-containing composition to metallic surface—4
JP H0748667 ASputtering target having high joining strength—24
US 5,403,458 ASputter-coating target and method of use199595
JP H07126837 AFormation of deposited film by bias sputtering—3
US 5,415,756 AIon assisted deposition process including reactive source gassification199564
JP H07235534 AManufacture of silicon wafer—19
US 5,464,520 ASilicide targets for sputtering and method of manufacturing the same199535
US 5,618,397 ASilicide targets for sputtering199735
US 5,639,311 AMethod of cleaning brushes used in post CMP semiconductor wafer cleaning operations199766
US 5,836,506 ASputter target/backing plate assembly and method of making same1998119
US 5,922,176 ASpark eliminating sputtering target and method for using and making same199954
EP 0,941,841 A2Method of lithographic imaging with reduced debris-generated performance degradation and related constructions—8
US 5,965,278 AMethod of making cathode targets comprising silicon199921
JP 2000021862 ASubstrate surface treating method and silicon semiconductor single crystal substrate—6
US 6,024,852 ASputtering target and production method thereof200038
US 6,030,514 AMethod of reducing sputtering burn-in time, minimizing sputtered particulate, and target assembly therefor200053
US 6,113,985 AProcess for the manufacture of group III nitride targets for use in sputtering and similar equipment200043
JP 2001059170 ASputtering target—19
JP 2001164361 ASputtering target cooling structure—15
US 6,283,357 B1Fabrication of clad hollow cathode magnetron sputter targets200171
US 6,284,111 B1Sputtering target free of surface-deformed layers200115
JP 3,226,193 B2シリコンウェーハの製造方法20012
US 6,342,134 B1Method for producing piezoelectric films with rotating magnetron sputtering system200225

Non-Patent Literature (5)

  • English translation of Information Statement from JPO issued in Japanese Application No. 2014-540207 filed May 2, 2014, Feb. 25, 2016.
  • English Translation of the Comments of the Examiner and the Search Report, The Patent Office of the People's Republic of China, issued May 21, 2015 in CN 201280054872.5 filed Nov. 7, 2012.
  • English Translation of the Comments of the Examiner and the Search Report, The Patent Office of the People's Republic of China, issued Nov. 23, 2015 in CN 201280054872.5 filed Nov. 7, 2012.
  • English Translation of the Comments of the Examiner, The Patent Office of the People's Republic of China, issued Mar. 7, 2016 in CN 201280054872.5 filed Nov. 7, 2012.
  • English translation of the Examination Report from Taiwan Intellectual Property Office issued on Apr. 21, 2016 in Taiwanese Application No. 101141269 filed Nov. 7, 2012.